Nickel plating was already routine by 1900, and it had one flaw: nickel yellows and dulls as it oxidises. Chromium does not — it holds a blue-white mirror indefinitely and is far harder than nickel. Everyone knew that. Nobody could deposit it.

Chromium plates out of chromic acid, and a pure chromic acid bath simply does not work: it deposits nothing, or a grey powder that brushes off. Dozens of chemists failed on it for thirty years.

Colin G. Fink found the missing piece — a catalyst anion. A small, precisely controlled quantity of sulphate must be present, at roughly 100 parts chromic acid to 1 part sulphate. Too little and nothing deposits; too much and nothing deposits. The window is narrow and it is the entire invention. His patent is US 1,581,188, "Process of Electrodepositing Chromium and of Preparing Baths Therefor", filed 19 December 1925 and granted 20 April 1926, later assigned to United Chromium, Inc.

Within five years every American car carried chrome, and the 1930s look — chrome bumpers, chrome grilles, chrome trim — exists because of a ratio.

⚠ This process uses hexavalent chromium, a confirmed human carcinogen. It is documented here because it is historically decisive and because omitting dangerous processes leaves holes in the record — not because it should be attempted outside professional containment. Read the safety step before anything else.

高级
2 hours

危险内容

此蓝图包含危险操作。请登录并在账户设置中启用危险内容,以查看分步说明。

相关蓝图

这些蓝图共享知识——技术、材料或原理

CC0 公共领域

此蓝图以 CC0 协议发布。你可以自由复制、修改、分发和使用此作品,无需征得许可。

通过购买蓝图中的产品支持创客,他们将获得 创客佣金 (由供应商设定),或创建此蓝图的新版本并将其作为连接包含在你自己的蓝图中以分享收入。

讨论

(0)

登录 加入讨论

加载评论中...