Germanium: Germanium Dioxide Reduced with Carbon at Full Red Heat, Fused under Borax (Roscoe 1913)
Charlie

创建者

Charlie

1. 十一月 2026DE
0
0
0
0
0

Germanium: Germanium Dioxide Reduced with Carbon at Full Red Heat, Fused under Borax (Roscoe 1913)

Carbon takes the oxygen from germanium dioxide at a full red heat. Washing removes the leftover carbon and a little borax melts the regulus clean. Result: greyish-white, brittle, lustrous germanium (sp. gr. 5.47, melts about 960 °C), often in octahedra. Source: Roscoe and Schorlemmer, A Treatise on Chemistry vol. 2 (1913), p. 838. Not given: amounts and vessel. Picture drawn by Youblob.
中级
1 day

说明

1

Reduce with carbon at full red heat

Heat germanium dioxide with carbon to a full red heat. Ours: powdered charcoal in a clay crucible.

此步骤所需材料:

二氧化锗二氧化锗1 as required

所需工具:

木炭木炭
石制研钵与研杵石制研钵与研杵
耐火黏土坩埚耐火黏土坩埚
坩埚炉坩埚炉
坩埚钳坩埚钳
2

Wash out the carbon

Wash the semi-crystalline regulus with water to remove the carbon.

所需工具:

水水
玻璃烧杯玻璃烧杯
3

Fuse with a little borax

Fuse the metal with a little borax.

所需工具:

硼砂粉硼砂粉
耐火黏土坩埚耐火黏土坩埚
坩埚炉坩埚炉
坩埚钳坩埚钳

材料

1

所需工具

8

此蓝图制作