Tinned Copper Wire: Boiled with Cream of Tartar and Grain Tin (Spon's Workshop Receipts)
Copper wire tinned without melting any tin: grain tin or tin shavings are boiled with cream of tartar and water, and the copper boiled in the same liquor until tin comes down on it as metal.
Spon gives the receipt for copper and brass in general. Here the copper is wire. Not given: how long to boil.
Source: Spon, Workshop Receipts, first series, p. 336. Picture: the receipt.
初学者
Unknown
说明
1
1
Boil the tinning liquor
Boil the tinning liquor
Boil 6 lb of cream of tartar, 4 gallons of water and 8 lb of grain tin or tin shavings together for a sufficient time. Ours: a clay pot as the vessel.
此步骤所需材料:
酒石1 6 lb
水1 4 gallons
锡锭1 8 lb, as grain or shavings所需工具:
陶罐2
2
Boil the wire in it
Boil the wire in it
Put the copper wire into the liquor and keep it boiling. The tin is precipitated on the copper in its metallic form.
此步骤所需材料:
铜线1 个所需工具:
陶罐此蓝图制作
CC0 公共领域
此蓝图以 CC0 协议发布。你可以自由复制、修改、分发和使用此作品,无需征得许可。