Barium-Lead Ferrite Disc Magnet: 0.35 mol BaCO3 and 0.3 mol PbO2, 1145 °C (Went, Philips 1956, Ex. 32)
A ceramic magnet with both barium and lead: 0.35 mol barium carbonate and 0.3 mol lead dioxide to 3.4 mol iron oxide, milled 15.5 hours, presintered by heating slowly to 900 °C, pressed and passed through a 1145 °C furnace in 4 minutes. Went's rod held 1,785 gauss with a coercive force of 2,840 oersted. Barium and lead compounds are poisonous.
Source: J. J. Went, G. W. van Oosterhout and E. W. Gorter (Philips), US 2,762,777 (1956), Example 32. They sintered rods; discs and the magnetising are ours. Picture: ferrite magnets, Omegatron, Wikimedia Commons, CC BY-SA 3.0.
Erfahren
2 days
Gefährlicher Inhalt
Dieser Blueprint enthält gefährliche Verfahren. Melden Sie sich an und aktivieren Sie gefährliche Inhalte in Ihren Kontoeinstellungen, um die Schritt-für-Schritt-Anleitung anzuzeigen.
AnmeldenDieser Bauplan stellt her
Verwandte Blueprints
Diese Blueprints teilen Wissen — Techniken, Materialien oder Prinzipien
CC0 Gemeinfrei
Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.
Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.