Charcoal Air Furnace for Crucibles, Drawn by a Chimney

The chemist's furnace for melting in crucibles needs no bellows: a firebrick box closed on every side, air entering only under the grate, and a tall chimney to draw it through the burning charcoal. George Fownes (1856) describes it; a sliding damper in the flue sets the heat, from dull red upward. The picture: a 16th-century assay workshop woodcut with wind furnaces, one on a tripod, for melting silver in crucibles (Deutsche Fotothek).
Fortgeschritten
Two days, plus drying

Anweisungen

1

Fireclay mortar

Mix fireclay and fine sand with water to a stiff, smooth mortar (our mix: about one part clay to one of sand).

Materialien für diesen Schritt:

SchamottetonSchamotteton10 kg
Feiner SandFeiner Sand10 kg
WasserWasser8 Liter

Benötigte Werkzeuge:

EimerEimer
HandschaufelHandschaufel
2

Ash pit and grate

Lay a level firebrick base and build a low ash pit with an opening at the front. Forge bars from wrought iron rod and set them across the top as the grate, a finger's width apart.

Materialien für diesen Schritt:

SchamottesteineSchamottesteine20 Stück
Schmiedeeiserne RundstangeSchmiedeeiserne Rundstange2 m

Benötigte Werkzeuge:

HandschaufelHandschaufel
WasserwaageWasserwaage
SchmiedeesseSchmiedeesse
KreuzschlaghammerKreuzschlaghammer
3

Fire box

Build a square box of firebricks on the grate, wide enough for a crucible with a hand's width of charcoal all round, and tall enough to cover it. Joint every brick thinly with the fireclay mortar.

Materialien für diesen Schritt:

SchamottesteineSchamottesteine40 Stück

Benötigte Werkzeuge:

HandschaufelHandschaufel
WasserwaageWasserwaage
4

Flue, chimney and damper

Lead a flue out near the top into a tall chimney pipe. Fit an iron sliding plate across the flue as a damper. Close the top with a loose firebrick lid.

Materialien für diesen Schritt:

RauchrohrRauchrohr1 Stück
Eisenblech (geschmiedet)Eisenblech (geschmiedet)1 Stück

Benötigte Werkzeuge:

HandschaufelHandschaufel
5

Dry and first fire

Let the mortar dry for days, then light a small charcoal fire and raise it slowly over an hour or two so the joints do not crack.

Materialien für diesen Schritt:

HolzkohleHolzkohle10 kg

Benötigte Werkzeuge:

Hitzebeständige HandschuheHitzebeständige Handschuhe
6

Draught from the chimney

Jupyter-Notebook wird geladen …
7

Limits

The principle and the damper are Fownes's; the sizes, the mortar mix and the draught formula's working figures are ours. Charcoal fires make carbon monoxide: work outdoors or under a good chimney.

Materialien

8

Benötigte Werkzeuge

6

Verwandte Blueprints

Diese Blueprints teilen Wissen — Techniken, Materialien oder Prinzipien

CC0 Gemeinfrei

Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.

Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.

Diskussion

(0)

Anmelden um an der Diskussion teilzunehmen

Kommentare werden geladen...