Clamping Caul: Zinc Plate with a Pine Backing Board (Adamson, 1889)

A caul spreads clamping pressure evenly over glued work. D. Adamson (1889) prefers zinc for veneering cauls because it lasts longer than wood: a plate 1/8 to 1/4 in. thick (1/8 in. is enough), with a loose backing board of sound pine about 1 in. thick that keeps it flat and holds its heat. Only the zinc is warmed; the pine backing goes on cold. Source: D. Adamson, "Practical Veneering", Work, 5 October 1889, pp. 453-455.
Anfänger
Unknown

Anweisungen

1

Read Adamson

"Perhaps as a general thing the zinc is usually preferred of from 1/8 in. to 1/4 in. in thickness, the former being quite sufficient for ordinary purposes. ... Even with a zinc caul a backing of wood is necessary to keep it flat down to the work, and to prevent the heat from dispersing too rapidly."
2

Cut the zinc

Cut a zinc plate 1/8 in. thick (1/8 to 1/4 in. is usual; too thin does not hold the heat, thicker is only waste), large enough to cover the surface to be pressed and lying flat. Length and width are set by the work (not given). How it is cut is not given (ours: tin snips).

Materialien für diesen Schritt:

ZinkblechZinkblech1 1/8 in.

Benötigte Werkzeuge:

BlechschereBlechschere
Unbekannte MaßeUnbekannte Maße
3

Make the backing board

Cut a backing board of good sound pine about 1 in. thick, the size of the zinc, and plane it flat so it keeps the zinc flat down to the work (ours: plane and straightedge).

Materialien für diesen Schritt:

KiefernbrettKiefernbrett1 about 1 in. thick

Benötigte Werkzeuge:

TischlersägeTischlersäge
HandhobelHandhobel
HaarlinealHaarlineal
4

Use it

Warm the zinc only (not so hot that it cannot be comfortably handled), lay it over the veneer with a sheet of slightly greased paper between, put the cold pine board on top, and screw down the hand-screws evenly until the glue oozes out at the edges. Leave it until the zinc is cold, an hour or two.

Benötigte Werkzeuge:

SchraubzwingenSchraubzwingen

Materialien

2
  • 1 1/8 in.
    Platzhalter
  • 1 about 1 in. thick
    Platzhalter

Benötigte Werkzeuge

6

CC0 Gemeinfrei

Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.

Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.

Diskussion

(0)

Anmelden um an der Diskussion teilzunehmen

Kommentare werden geladen...