Forged Ball-Peen Hammer
A 2-pound ball-peen hammer forged from 1½-inch square tool steel; a 6½-inch bar gives two heads. The eye is punched and drifted, the body fullered and rounded so it tapers both ways from a thick centre, then the face is drawn out and swaged and the ball peen rounded in a bottom swage. Both ends are hardened by dipping them in turn, with water dripping on the face, and tempered from the heat held around the eye: dark brown for the face, brown or purple for the peen. The eye cools last, which keeps it tough.
Erfahren
4–6 hours
Anweisungen
1
1
Mark and flatten
Mark and flatten
Mark the bar with a chisel and centre punch. Flatten the end before punching, or the hole grows too large.
Materialien für diesen Schritt:
Werkzeugstahl-Vierkantstab1 StückBenötigte Werkzeuge:
Körner
Warmschrotmeißel
Schmiedeesse
Amboss
Vorschlaghammer
Schmiedezange2
2
Punch and drift the eye
Punch and drift the eye
Punch the eye at the centre-punch mark, drive in a drift and hammer the bulged sides straight.
Benötigte Werkzeuge:
Warmlocheisen
Lochdorn
Schmiedehammer3
3
Shape the body
Shape the body
Rough out the shape with top and bottom fullers, then round the body at the anvil's rounded edge with a top fuller and set hammer, thicker at the centre than at the ends.
Benötigte Werkzeuge:
Fuller (Ausbreitgesenk)
Setzhammer4
4
Face and peen
Face and peen
Cut the head from the bar from four sides for a square end. Draw out the face, swage it and trim it with a hot chisel; then cut the peen to length, cut off its corners and round it in a bottom swage. Drive the drift through from both sides to taper the eye.
Benötigte Werkzeuge:
Warmschrotmeißel
Untergesenk
Lochdorn5
5
Grind
Grind
Grind both ends, rounding the edges of the face slightly so it does not mark hot work.
Benötigte Werkzeuge:
Doppelschleifer6
6
Harden and temper
Harden and temper
Heat the whole head slowly to the hardening heat and hold it by a tong jaw in the eye. Lower about 1½ inches of the face into water, then harden the peen the same way while water drips on the face, keeping the eye hot. Polish the ends; take the face to dark brown and the peen to brown or purple, then dip the ends alternately so the eye cools slowly.
Benötigte Werkzeuge:
Schmiedeesse
Abschreckbottich
Schmiedezange
Schmirgelleinen7
7
Handle
Handle
Shave the handle stock to fit the eye tightly, drive the head on, saw a kerf in the handle's top and drive a glued hardwood wedge into it. Trim flush and oil the handle.
Materialien für diesen Schritt:
Hartholzstiel-Rohling1 Stück
Hartholzkeil1 Stück
Leinöl10 mlBenötigte Werkzeuge:
Schweifhobel
Zugsäge
SchraubstockMaterialien
4- 1 StückPlatzhalter
- 1 StückPlatzhalter
- 1 StückPlatzhalter
- 10 mlPlatzhalter
Benötigte Werkzeuge
18- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
- Platzhalter
Dieser Bauplan stellt her
Verwandte Blueprints
Diese Blueprints teilen Wissen — Techniken, Materialien oder Prinzipien
CC0 Gemeinfrei
Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.
Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.