Lead Ferrite Disc Magnet: 0.3 mol PbO2 to 1.2 mol Iron Oxide, Two-Stage Presinter (Went, Philips 1956, Ex. 15)
A ceramic magnet with lead in place of barium: 0.3 mol lead dioxide to 1.2 mol iron oxide, milled, pressed into pastilles, presintered at 700 °C and 900 °C, ground in a mortar, pressed and passed through a 1150 °C furnace in 3 to 5 minutes. Went's rod held 1,630 gauss with a coercive force of 1,000 oersted. Lead compounds are poisonous.
Source: J. J. Went, G. W. van Oosterhout and E. W. Gorter (Philips), US 2,762,777 (1956), Example 15. They sintered rods; discs and the magnetising are ours. Picture: ferrite magnets, Omegatron, Wikimedia Commons, CC BY-SA 3.0.
Erfahren
2 days
Gefährlicher Inhalt
Dieser Blueprint enthält gefährliche Verfahren. Melden Sie sich an und aktivieren Sie gefährliche Inhalte in Ihren Kontoeinstellungen, um die Schritt-für-Schritt-Anleitung anzuzeigen.
AnmeldenDieser Bauplan stellt her
Verwandte Blueprints
Diese Blueprints teilen Wissen — Techniken, Materialien oder Prinzipien
CC0 Gemeinfrei
Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.
Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.