Plastic Extruder: Steam-Jacketed Screw Stuffer with a Heated Nozzle (Andersen & Strasdin, US 2,384,521, 1945)
Emma

Erstellt von

Emma

3. November 2026SE
5
0
0
0
0

Plastic Extruder: Steam-Jacketed Screw Stuffer with a Heated Nozzle (Andersen & Strasdin, US 2,384,521, 1945)

A screw extruder for thermoplastics: a turning screw in a steam-jacketed barrel pushes hot, softened plastic forward through a short nozzle heated electrically. The barrel is kept a little below the plastic's flow temperature and the nozzle well above it, so the extruded rod comes out with a smooth, glass-like skin. Result: an extruder that makes rod, tube or strip at 25 to 30 feet a minute. Source: B. Andersen and R. F. Strasdin (Celanese), US 2,384,521 (1945). Unknown: sizes and metals. Picture: the patent drawing.
Erfahren
Unknown

Anweisungen

1

Make the screw

Turn a screw to fit the barrel. Its thread may be single or double; to press the plastic harder toward the nozzle, make the pitch increase or the groove get shallower toward that end. Example: a double-thread screw. Ours: mild steel. Not given: sizes.

Materialien für diesen Schritt:

Rundstahl aus BaustahlRundstahl aus Baustahl1 screw

Benötigte Werkzeuge:

MetalldrehmaschineMetalldrehmaschine
FräsmaschineFräsmaschine
Unbekannte MaßeUnbekannte Maße
2

Make the jacketed barrel

Make the barrel with a steam jacket round it and a steam port into the jacket, and a feed throat at the back end. The inside wall may be grooved, pitched so that every flight of the screw always meets a groove; this stops the plastic slipping. Not given: the metal, the steam pressure.

Materialien für diesen Schritt:

Unbekanntes MetallUnbekanntes Metall1 barrel and jacket

Benötigte Werkzeuge:

MetalldrehmaschineMetalldrehmaschine
Unbekannte MaßeUnbekannte Maße
3

Fit the heated nozzle

At the front, fit a streamlined nozzle head so no plastic can pocket and decompose, and a nozzle 1/2 to 18 inches long; about 6 inches in the example. Perforated plates may go between the screw and the nozzle. Heat the nozzle with an electric resistance coil. Ours: nichrome wire.

Materialien für diesen Schritt:

Unbekanntes MetallUnbekanntes Metall1 nozzle head and nozzle
NichromdrahtNichromdraht1 nozzle heating coil
Unbekannter IsolierstoffUnbekannter Isolierstoff1 coil insulation

Benötigte Werkzeuge:

MetalldrehmaschineMetalldrehmaschine
4

Drive the screw

Drive the screw through a gear from a motor, so its speed can be kept steady; 20 revolutions a minute in the example. Not given: the drive.

Materialien für diesen Schritt:

ElektromotorElektromotor1 drive motor
Unbekanntes MetallUnbekanntes Metall1 drive gears

Benötigte Werkzeuge:

Unbekannte MaßeUnbekannte Maße
5

Extrude a rod

Keep the barrel 0 to 100 °F below the plastic's flow temperature and the nozzle 50 to 100 °F above it. Example: barrel at about 270 °F by steam, nozzle at about 400 °F, for a cellulose acetate with a flow temperature of 307 °F. Feed the hot, softened plastic into the throat at a steady rate. Carry the rod away on a conveyor and cool it at once with cold water, then cut it to length.

Benötigte Werkzeuge:

DampfkesselDampfkessel
PyrometerPyrometer
WasserWasser

Materialien

5

Benötigte Werkzeuge

6

CC0 Gemeinfrei

Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.

Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.

Diskussion

(0)

Anmelden um an der Diskussion teilzunehmen

Kommentare werden geladen...