Potassium bromide is the bromide of photography. Thorpe (1913): iron bromide solution run into hot potash solution until it is just neutral throws down the iron as oxide and leaves potassium bromide in solution, which is filtered, evaporated and crystallised. 100 parts of iron bromide take 56 to 60 parts of potash. The picture: potassium bromide crystals (Wikimedia Commons).
Fortgeschritten
2 days

Anweisungen

1

Make the two solutions

Dissolve the iron bromide in water and filter it. Dissolve 56 to 60 g of potash, according to its purity, in a little water and heat it.

Materialien für diesen Schritt:

EisenbromidEisenbromid100 g
Kaliumcarbonat (Pottasche)Kaliumcarbonat (Pottasche)60 g

Benötigte Werkzeuge:

WasserWasser
Grobes BaumwollfiltertuchGrobes Baumwollfiltertuch
Gusseiserner TopfGusseiserner Topf
BalkenwaageBalkenwaage
2

Run the iron bromide into the potash

Pour the iron bromide solution into the hot potash until the liquid is exactly neutral or very faintly alkaline. Iron oxide falls out.

Benötigte Werkzeuge:

Gusseiserner TopfGusseiserner Topf
LackmuspapierLackmuspapier
GummihandschuheGummihandschuhe
3

Boil and filter

Boil for some time so the iron oxide settles dense, then filter it off.

Benötigte Werkzeuge:

Gusseiserner TopfGusseiserner Topf
Grobes BaumwollfiltertuchGrobes Baumwollfiltertuch
4

Dry, then dissolve again

Evaporate to dryness. Dissolve the residue again in water: potassium sulphate and other dirt stay behind. Filter.

Benötigte Werkzeuge:

Gusseiserner TopfGusseiserner Topf
WasserWasser
Grobes BaumwollfiltertuchGrobes Baumwollfiltertuch
5

Crystallise

Boil down to specific gravity 1.53, then evaporate further at a gentle heat in a stoneware or enamelled dish, for hard crystals.

Benötigte Werkzeuge:

Gusseiserner TopfGusseiserner Topf
Spindel (Aräometer)Spindel (Aräometer)
AbdampfschaleAbdampfschale
6

Dry at 40 to 50 °C

Dry the crystals at 40 to 50 °C, not above, or they crackle and burst.

Benötigte Werkzeuge:

AbdampfschaleAbdampfschale
ThermometerThermometer

Materialien

2

Benötigte Werkzeuge

9

Dieser Bauplan stellt her

Verwandte Blueprints

Diese Blueprints teilen Wissen — Techniken, Materialien oder Prinzipien

CC0 Gemeinfrei

Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.