Tungsten Powder: Wolfram Fused with Soda, Tungstic Acid Reduced with Carbon in Crucibles (Oxland Process, Thorpe 1913)
How tungsten powder for steelmakers was made: wolfram is roasted with soda to sodium tungstate (Oxland's process of 1847), the tungstate is poured into boiling hydrochloric acid to throw down tungstic acid, and that is reduced with a little less than its carbon in crucibles. Washing takes off the free carbon and the finest dust.
Result: fine-grained, granular tungsten powder, usually over 98 % tungsten with about 0.5 % each of iron and silicon and under 0.5 % carbon.
Source: Thorpe, A Dictionary of Applied Chemistry vol. 5 (1913), pp. 564-565. Not given: crucible, reduction temperature and time, the vessels for the acid. Boiling hydrochloric acid is a strong acid. Picture drawn by Youblob.
Erfahren
1 week
Gefährlicher Inhalt
Dieser Blueprint enthält gefährliche Verfahren. Melden Sie sich an und aktivieren Sie gefährliche Inhalte in Ihren Kontoeinstellungen, um die Schritt-für-Schritt-Anleitung anzuzeigen.
AnmeldenDieser Bauplan stellt her
Verwandte Blueprints
Diese Blueprints teilen Wissen — Techniken, Materialien oder Prinzipien
CC0 Gemeinfrei
Dieser Blueprint ist unter CC0 veröffentlicht. Sie dürfen dieses Werk für jeden Zweck frei kopieren, ändern, verbreiten und verwenden, ohne um Erlaubnis zu fragen.
Unterstützen Sie den Maker, indem Sie Produkte über seinen Blueprint kaufen, wo er eine Maker-Provision von Anbietern festgelegt, verdient. Oder erstellen Sie eine neue Iteration dieses Blueprints und verbinden Sie ihn in Ihrem eigenen Blueprint, um Einnahmen zu teilen.