Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Methanol
Philips' Ponjee and Verwijlen (US 4,639,382, 1987) made silver hold on acrylic by first dipping it in tannin dissolved in water mixed with an organic solvent; tannin in plain water gave no bond. This is their methanol solution: 45–70 % water, 30–55 % methanol by volume, 2.7–4.3 g tannin per litre, which gave full bonding in their cross-cut test. The sheet is then sensitised with weak stannous chloride and silvered by spraying the silver solution and the reducer together.
The picture: our diagram.
Intermedio
2 hours
Instrucciones
1
1
Dip in tannin solution for one minute
Dip in tannin solution for one minute
Make a solution of 2.7–4.3 g of tannic acid per litre in 45–70 % water and 30–55 % methanol by volume. Dip the acrylic sheet in it for one minute.
Materiales para este paso:
Lámina de acrílico1 piezaHerramientas necesarias:
Ácido tánico
Metanol
Agua destilada
Bandejas de vidrio
Probeta graduada
Balanza de platillos
Campana extractora (con conducto)
Guantes de goma2
2
Rinse with water
Rinse with water
Rinse the sheet with water.
Herramientas necesarias:
Agua destilada
Frasco lavador de laboratorio3
3
Spray with stannous chloride for 12 seconds
Spray with stannous chloride for 12 seconds
Spray the face to be silvered with a solution of 0.1 g stannous chloride and 0.1 ml concentrated hydrochloric acid per litre of water, for 12 seconds. Rinse off the excess with water.
Herramientas necesarias:
Cloruro estannoso
Ácido clorhídrico
Agua destilada
Pulverizador de agua
Frasco lavador de laboratorio
Gafas de protección química
Guantes de goma4
4
Spray silver and reducer together
Spray silver and reducer together
Atomise two solutions onto the face at the same time: silver nitrate with ammonia in water, and formalin in water. The patent gives no strengths: as required. Ours: a twin-nozzle spray gun.
Materiales para este paso:
Nitrato de plata1 as requiredHerramientas necesarias:
Disolución de amoníaco al 25-28 %
Disolución de formaldehído (formol al 37 %)
Agua destilada
Pistola de pulverización de doble boquilla
Campana extractora (con conducto)
Gafas de protección química
Guantes de gomaMateriales
2- 1 piezaMarcador de posición
- 1 as requiredMarcador de posición
Herramientas requeridas
16- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
Este plano hace
Blueprints relacionados
Estos blueprints comparten conocimiento — técnicas, materiales o principios
CC0 Dominio público
Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.
Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.