Aluminium Hydroxide: Alum Solution Dropped into Ammonia Water (Ure 1839)
Drop a weak alum solution into ammonia water and a bulky white precipitate falls: aluminium hydroxide, which Ure called aluminous earth. Washed, it is the starting point for aluminium salts and for alumina.
Result: a bulky white precipitate; dried, it weighs 10.82 % of the alum used. Ure dissolves it in acid while it is still moist.
Source: Ure, Dictionary of Arts, Manufactures, and Mines (1839), Alum. Not given: how much ammonia water, its strength, how it is washed. Ours: work in fresh air, as ammonia fumes sting. Picture drawn by Youblob.
Principiante
3 hours
Instrucciones
1
1
Dissolve alum in 20 parts of water
Dissolve alum in 20 parts of water
Weigh the alum and dissolve it in 20 times its weight of water.
Materiales para este paso:
Alumbre (alumbre potásico)1 part by weightHerramientas necesarias:
Agua destilada
Balanza de platillos
Vaso de precipitados de borosilicato
Varilla de vidrio2
2
Drop it slowly into ammonia water
Drop it slowly into ammonia water
Drop the alum solution slowly into caustic ammonia water, stirring, until the ammonia is nearly, but not entirely, saturated. A bulky white precipitate falls down. Ure gives no strength. Ours: 25-28 % ammonia solution.
Herramientas necesarias:
Disolución de amoníaco al 25-28 %
Vaso de precipitados de borosilicato
Varilla de vidrio3
3
Wash the precipitate with water
Wash the precipitate with water
Wash the precipitate properly with water. Ure does not say how. Ours: collect it on filter paper in a funnel and pour water through until the washings no longer smell of ammonia.
Herramientas necesarias:
Embudo de vidrio con vástago
Papel de filtro
Agua destilada4
4
Keep it moist for dissolving
Keep it moist for dissolving
Dried, the precipitate weighs 10.82 % of the alum. Ure dissolves it in acid while it is still moist. Ours: keep it wet in a closed jar until it is used.
Herramientas necesarias:
Tarros de vidrio con tapaMateriales
1- 1 part by weightMarcador de posición
Herramientas requeridas
8- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
- Marcador de posición
Este plano hace
Blueprints relacionados
Estos blueprints comparten conocimiento — técnicas, materiales o principios
CC0 Dominio público
Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.
Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.