Carbon Resistance Ring: Laminated Paper Gelled with 15% Tung Oil, Graphite-Shellac Track
Ed

Creado por

Ed

21. octubre 2026FI
5
0
0
0
0

Carbon Resistance Ring: Laminated Paper Gelled with 15% Tung Oil, Graphite-Shellac Track

Mallory's quiet volume-control ring (US 2,144,925, 1939). Hard bases were noisy and soft paper ones changed with damp. Their answer: paper rings soaked in 15 % raw tung oil and baked, so the oil gels inside the paper. It shuts out moisture but stays soft and springy, and the wiper runs on it quietly. A graphite paint makes the track, silver paint the ends. The picture: the patent's drawing (Fig. 3).
Intermedio
1 day

Instrucciones

1

Punch rings from three-ply paper

The base is three papers stuck into one sheet: litho paper at the back, newsprint in the middle, manila on the face that takes the track. Punch rings from it. Ours: a punch press with a ring die.

Materiales para este paso:

Papel laminado de tres capasPapel laminado de tres capas1 pieza

Herramientas necesarias:

Prensa punzonadoraPrensa punzonadora
Troquel para anillosTroquel para anillos
Guantes de gomaGuantes de goma
2

Soak 1 hour in 15 % tung oil in naphtha

Soak the rings for about one hour in about 15 % raw tung oil in naphtha. Use raw oil, not heat-bodied or treated oil, so it can still gel.

Materiales para este paso:

Aceite de tungAceite de tung15 parts

Herramientas necesarias:

NaftaNafta
Vaso de precipitados de vidrioVaso de precipitados de vidrio
Balanza de platillosBalanza de platillos
AgitadorAgitador
Máscara respiratoria de cara completaMáscara respiratoria de cara completa
Guantes de gomaGuantes de goma
3

Air-dry, then bake at 210–250 °C

Dry the rings in air for two hours or more, then bake 15 to 30 minutes at 210 to 250 °C. The oil gels in the paper's pores; the paper stays pliable.

Herramientas necesarias:

Horno de secadoHorno de secado
Termómetro de hornoTermómetro de horno
Guantes resistentes al calorGuantes resistentes al calor
4

Spray the graphite track

Spray on the resistance paint, for example graphite in a shellac binder. The patent gives no proportions. The track can be tapered in thickness, width or mix to shape the resistance curve.

Materiales para este paso:

Polvo de grafitoPolvo de grafito1 as required
Goma lacaGoma laca1 as required

Herramientas necesarias:

Pistola de pinturaPistola de pintura
Compresor de aireCompresor de aire
Máscara respiratoria de cara completaMáscara respiratoria de cara completa
Guantes de gomaGuantes de goma
5

Paint silver ends, bake at 220 °C

Spray or paint the two end terminals with silver particles in shellac. Dry, then bake at about 220 °C to cure and harden the track. The slight warp from soaking flattens out again.

Materiales para este paso:

Pintura conductora de plataPintura conductora de plata1 as required

Herramientas necesarias:

Pistola de pinturaPistola de pintura
Horno de secadoHorno de secado
Termómetro de hornoTermómetro de horno
Guantes resistentes al calorGuantes resistentes al calor

Materiales

5

Herramientas requeridas

13

CC0 Dominio público

Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.

Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.

Discusión

(0)

Iniciar sesión para unirte a la discusión

Cargando comentarios...