Clamping Caul: Zinc Plate with a Pine Backing Board (Adamson, 1889)
Woody

Creado por

Woody

9. noviembre 2026NO
2
0
0
0
0

Clamping Caul: Zinc Plate with a Pine Backing Board (Adamson, 1889)

A caul spreads clamping pressure evenly over glued work. D. Adamson (1889) prefers zinc for veneering cauls because it lasts longer than wood: a plate 1/8 to 1/4 in. thick (1/8 in. is enough), with a loose backing board of sound pine about 1 in. thick that keeps it flat and holds its heat. Only the zinc is warmed; the pine backing goes on cold. Source: D. Adamson, "Practical Veneering", Work, 5 October 1889, pp. 453-455.
Principiante
Unknown

Instrucciones

1

Read Adamson

"Perhaps as a general thing the zinc is usually preferred of from 1/8 in. to 1/4 in. in thickness, the former being quite sufficient for ordinary purposes. ... Even with a zinc caul a backing of wood is necessary to keep it flat down to the work, and to prevent the heat from dispersing too rapidly."
2

Cut the zinc

Cut a zinc plate 1/8 in. thick (1/8 to 1/4 in. is usual; too thin does not hold the heat, thicker is only waste), large enough to cover the surface to be pressed and lying flat. Length and width are set by the work (not given). How it is cut is not given (ours: tin snips).

Materiales para este paso:

Chapa de cincChapa de cinc1 1/8 in.

Herramientas necesarias:

Tijeras de chapaTijeras de chapa
Dimensiones desconocidasDimensiones desconocidas
3

Make the backing board

Cut a backing board of good sound pine about 1 in. thick, the size of the zinc, and plane it flat so it keeps the zinc flat down to the work (ours: plane and straightedge).

Materiales para este paso:

Tabla de pinoTabla de pino1 about 1 in. thick

Herramientas necesarias:

Serrucho de carpinteroSerrucho de carpintero
Cepillo de carpinteroCepillo de carpintero
Regla de trazarRegla de trazar
4

Use it

Warm the zinc only (not so hot that it cannot be comfortably handled), lay it over the veneer with a sheet of slightly greased paper between, put the cold pine board on top, and screw down the hand-screws evenly until the glue oozes out at the edges. Leave it until the zinc is cold, an hour or two.

Herramientas necesarias:

SargentosSargentos

Materiales

2
  • 1 1/8 in.
    Marcador de posición
  • 1 about 1 in. thick
    Marcador de posición

Herramientas requeridas

6

CC0 Dominio público

Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.

Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.

Discusión

(0)

Iniciar sesión para unirte a la discusión

Cargando comentarios...