LDPE Pellets: Ethylene Polymerised at 1500 Atmospheres with a Trace of Oxygen
Polyethylene was discovered at ICI by Fawcett, Gibson and Perrin (US 2,153,553, 1939): ethylene squeezed to over a thousand atmospheres and heated, with a trace of oxygen to start the reaction, turns into a tough, waxy solid that melts at about 120 °C. Their Example III, at 1500 atmospheres and 210 °C for 5 hours, turned 80 % of the ethylene into polymer. The heat of reaction must be carried away, or the gas decomposes explosively. Extruding it into pellets is our step.
The picture: our diagram.
Avanzado
About 6 hours
Contenido peligroso
Este blueprint contiene procedimientos peligrosos. Inicia sesión y habilita el contenido peligroso en la configuración de tu cuenta para ver las instrucciones paso a paso.
Iniciar sesiónEste plano hace
Blueprints relacionados
Estos blueprints comparten conocimiento — técnicas, materiales o principios
CC0 Dominio público
Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.
Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.