Carbon Resistance Ring: Laminated Paper Gelled with 10% Tung Oil, Graphite-Shellac Track
Ed

Créé par

Ed

21. octobre 2026FI
11
0
0
0
0

Carbon Resistance Ring: Laminated Paper Gelled with 10% Tung Oil, Graphite-Shellac Track

Mallory's quiet volume-control ring (US 2,144,925, 1939). Hard bases were noisy and soft paper ones changed with damp. Their answer: paper rings soaked in 10 % raw tung oil and baked, so the oil gels inside the paper. It shuts out moisture but stays soft and springy, and the wiper runs on it quietly. A graphite paint makes the track, silver paint the ends. The picture: the patent's drawing (Fig. 3).
Intermédiaire
1 day

Consignes

1

Punch rings from three-ply paper

The base is three papers stuck into one sheet: litho paper at the back, newsprint in the middle, manila on the face that takes the track. Punch rings from it. Ours: a punch press with a ring die.

Matériaux pour cette étape :

Papier stratifié à trois couchesPapier stratifié à trois couches1 pièce

Outils nécessaires :

Presse à poinçonnerPresse à poinçonner
Matrice à découper les anneauxMatrice à découper les anneaux
Gants en caoutchoucGants en caoutchouc
2

Soak 1 hour in 10 % tung oil in naphtha

Soak the rings for about one hour in about 10 % raw tung oil in naphtha. Use raw oil, not heat-bodied or treated oil, so it can still gel.

Matériaux pour cette étape :

Huile de tungHuile de tung10 parts

Outils nécessaires :

NaphtaNaphta
Bécher en verreBécher en verre
Balance à fléauBalance à fléau
AgitateurAgitateur
Masque respiratoire completMasque respiratoire complet
Gants en caoutchoucGants en caoutchouc
3

Air-dry, then bake at 210–250 °C

Dry the rings in air for two hours or more, then bake 15 to 30 minutes at 210 to 250 °C. The oil gels in the paper's pores; the paper stays pliable.

Outils nécessaires :

Étuve de séchageÉtuve de séchage
Thermomètre de fourThermomètre de four
Gants résistants à la chaleurGants résistants à la chaleur
4

Spray the graphite track

Spray on the resistance paint, for example graphite in a shellac binder. The patent gives no proportions. The track can be tapered in thickness, width or mix to shape the resistance curve.

Matériaux pour cette étape :

Poudre de graphitePoudre de graphite1 as required
Gomme laqueGomme laque1 as required

Outils nécessaires :

Pistolet à peinturePistolet à peinture
Compresseur d'airCompresseur d'air
Masque respiratoire completMasque respiratoire complet
Gants en caoutchoucGants en caoutchouc
5

Paint silver ends, bake at 220 °C

Spray or paint the two end terminals with silver particles in shellac. Dry, then bake at about 220 °C to cure and harden the track. The slight warp from soaking flattens out again.

Matériaux pour cette étape :

Peinture conductrice à l'argentPeinture conductrice à l'argent1 as required

Outils nécessaires :

Pistolet à peinturePistolet à peinture
Étuve de séchageÉtuve de séchage
Thermomètre de fourThermomètre de four
Gants résistants à la chaleurGants résistants à la chaleur

Matériaux

5

Outils requis

13

CC0 Domaine public

Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.

Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.

Commentaires

(0)

Se connecter pour participer à la discussion

Chargement des commentaires...