Continuous Glass Fibre Strand Drawn from a Platinum Bushing
Glass fibre for cloth is not spun like wool: hundreds of fine filaments are pulled at once from small nozzles in a hot platinum box and wound up as one strand. This is the method of Slayter and Thomas's Owens-Corning patent (US 2,234,986, 1941): an electrically heated platinum-rhodium thimble melts glass cullet, a blower freezes each filament just below its nozzle, a size is put on, and a drum pulls and winds the strand. The faster the drum, the finer the fibre.
The picture: a glass fibre roving (NoiseD, Wikimedia Commons, CC BY-SA 3.0).
Avancé
1 day
Consignes
1
1
Charge the bushing with cullet
Charge the bushing with cullet
Fill the platinum-rhodium thimble (90 % platinum, 10 % rhodium) with broken soda-lime glass. Its floor has rows of staggered nipples .02–.08 in (0.5–2 mm) wide; .04 in (1 mm) is best.
Matériaux pour cette étape :
Calcin de verre sodocalcique1 as requiredOutils nécessaires :
Filière en platine-rhodium
Gants résistants à la chaleur
Lunettes de sécurité2
2
Melt it with an electric current
Melt it with an electric current
Pass an adjustable current through the thimble to melt the glass. Ordinary lime glass is pulled from about 2,100–2,500 °F (about 1,150–1,370 °C).
Outils nécessaires :
Filière en platine-rhodium
Transformateur abaisseur
Pyromètre
Gants résistants à la chaleur3
3
Start the cooling blower
Start the cooling blower
Blow cool air across the nipple tips from a blower a short distance below them. Each filament sets within a small fraction of an inch of its nipple.
Outils nécessaires :
Soufflerie4
4
Gather the filaments through a sized guide
Gather the filaments through a sized guide
Draw all the filaments together through one guide eye kept wet with size. Here the size is wax, kept molten with a burner; the patent also names oil, starch, gum and resin. An air jet dries off the excess size.
Matériaux pour cette étape :
Paraffine1 as requiredOutils nécessaires :
Bec Bunsen
Soufflerie5
5
Pull and wind on a drum
Pull and wind on a drum
Wind the strand on a fast drum that moves back and forth so it lays evenly. Draw at a few hundred to a few thousand feet per minute: the faster you draw, the finer the fibre.
Outils nécessaires :
Tambour de réceptionMatériaux
2- 1 as requiredEspace réservé
- 1 as requiredEspace réservé
Outils requis
8- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
Ce plan fabrique
CC0 Domaine public
Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.
Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.