Platinum Reforming Catalyst: 0.1 % Platinum and 1.5 % Fluorine on Alumina (Haensel, UOP, US 2,479,110)
Haensel's reforming catalyst: a trace of platinum, only 0.1 %, on alumina that also carries fluorine. The fluorine is what makes it work: on the same naphtha it lifted the reformate from octane 59.8 to 78.8.
Variable: fluorine content. Tested on a Pennsylvania naphtha of octane 41.8: no fluorine 59.8; 1.5 % 78.8 (874 °F); 3 % 77.4 (824 °F); 6 % 72.4 (755 °F). Keep it at about 3 % or below.
Source: Haensel, US 2,479,110 (1949), Ex. I-II and IV. Not given: amounts of the aluminium salt and ammonia. Unknown: how the aluminium chloride hexahydrate, chloroplatinic acid and hydrogen sulfide are made. Danger: hydrofluoric acid and hydrogen sulfide are deadly poisons. Picture drawn by Youblob.
Expert
3 days
Contenu dangereux
Ce blueprint contient des procédures dangereuses. Connectez-vous et activez le contenu dangereux dans les paramètres de votre compte pour voir les instructions étape par étape.
Se connecterCe plan fabrique
Blueprints liés
Ces blueprints partagent des connaissances — techniques, matériaux ou principes
CC0 Domaine public
Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.
Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.