Saw File: Three-Square, Forged in a Boss, Cut by Hand and Hardened (Ure, 1839)
Forge

Créé par

Forge

4. novembre 2026NO
24
0
0
0
0

Saw File: Three-Square, Forged in a Boss, Cut by Hand and Hardened (Ure, 1839)

The file for sharpening saw teeth as Sheffield made it by hand: a three-square (triangular) bar of cast steel, not tapering, forged in a V-shaped boss, its teeth cut one by one with a chisel and hammer, then hardened under a coat of animal carbon and salt and quenched in cold spring water. Ure says saw files in particular should be hardened with the carbon mixture, so they will cut iron and steel. Not given: sizes and teeth per inch. Source: A. Ure, Dictionary of Arts, Manufactures, and Mines (1839), File. Picture: our drawing.
Avancé
Unknown

Consignes

1

Forge the blank

Draw cast steel out square at the forge, then lay it with one angle down in a boss whose recess has two sides meeting at an angle, so the hammer forms one side and the boss the other two. Keep it the same size along its length (saw files are not tapered).

Matériaux pour cette étape :

Acier au creusetAcier au creuset1 cast steel bar
Dimensions inconnuesDimensions inconnues1 pièce

Outils nécessaires :

Forge de forgeronForge de forgeron
Tenailles de forgeTenailles de forge
Étampe inférieureÉtampe inférieure
MarteauMarteau
MasseMasse
2

Cut the teeth

On an anvil with a flat, even face, hold the file down with a leather strap over each end, the workman's feet in the straps like stirrups. Cut the teeth with a chisel a little broader than the file, sharpened to about 20 degrees, struck with a hammer of 1 to 6 lb. For single cut, run a fine file lightly over the teeth to take off the roughness; for double cut, cut a second set nearly at right angles to the first.

Outils nécessaires :

Enclume en acierEnclume en acier
Lanière de cuirLanière de cuir
Burin à froidBurin à froid
MarteauMarteau
Lime à métauxLime à métaux
3

Cut the other sides

To cut the next side, lay the file in a piece of lead-tin alloy with an angular groove, so the teeth already cut are not spoiled on the anvil.

Outils nécessaires :

Soudure étain-plombSoudure étain-plomb
Enclume en acierEnclume en acier
Burin à froidBurin à froid
MarteauMarteau
4

Coat for hardening

Distil shoemakers' and curriers' leather refuse in an iron still and powder the bright coal left. Grind about equal parts by bulk of this carbon and salt to the consistence of cream with water and cover the file with it.

Outils nécessaires :

Cornue de ferCornue de fer
SelSel
EauEau
5

Harden

Hold the file by the tang in a fire of very small cokes, drawing it out often, until it is an even cherry red from tang to point. Plunge it straight down, quickly, into clear spring water as cold as possible.

Outils nécessaires :

Forge de forgeronForge de forgeron
Coke métallurgiqueCoke métallurgique
Tenailles de forgeTenailles de forge
EauEau
6

Clean and oil

Brush the file with water and powdered cokes until clean and metallic, wash it in two or three waters to take off all the salt, dip it in lime-water, dry it quickly before the fire and oil it while warm with olive oil containing a little oil of turpentine.

Outils nécessaires :

Coke métallurgiqueCoke métallurgique
EauEau
Eau de chauxEau de chaux
Huile d'oliveHuile d'olive
TérébenthineTérébenthine

Matériaux

2

Outils requis

17

CC0 Domaine public

Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.

Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.

Commentaires

(0)

Se connecter pour participer à la discussion

Chargement des commentaires...