Tannic Acid: Chinese Galls Extracted with Warm Water, Shaken with Ether and Dried on Tin Sheets
This is the large-scale way to make commercial tannin, as Thorpe's Dictionary (1913) gives it. Chinese galls from sumach hold as much as 70 % tannin; the best oak galls, from Aleppo, 50–60 %. The powder is extracted with warm water, and the extract is shaken with ether. After several days the ether layer on top is taken off; the tannin stays in the lower layer, which is dried on hot tin sheets until it puffs up. The product still holds some gallic acid, wax and glucose. Ether is very flammable: no flame.
The picture: our diagram.
Intermédiaire
1 week
Consignes
1
1
Extract the powdered galls with warm water
Extract the powdered galls with warm water
Powder Chinese galls finely. Stir with enough water at 50–60 °C to make a strong extract. Filter it clear.
Matériaux pour cette étape :
Noix de galle de Chine1 as requiredOutils nécessaires :
Eau
Mortier et pilon en pierre
Agitateur
Bain thermostaté
Thermomètre de laboratoire
Papier filtre
Entonnoir en verre à tige2
2
Shake with a quarter volume of ether
Shake with a quarter volume of ether
Add ether, one quarter of the extract's volume, and agitate until it forms an emulsion. Let it stand for several days.
Outils nécessaires :
Éther diéthylique
Ampoule à décanter à robinet
Sorbonne (à extraction)
Lunettes-masque anti-projections chimiques
Gants en caoutchouc3
3
Take off the ether layer and recover the ether
Take off the ether layer and recover the ether
Remove the upper ether layer. Run the lower layer, which holds all the tannin, into a still and distil off the ether in it to recover it. No flame near the ether.
Outils nécessaires :
Ampoule à décanter à robinet
Alambic en cuivre
Sorbonne (à extraction)4
4
Dry on tin sheets over a steam coil
Dry on tin sheets over a steam coil
Let the syrupy liquid cool, spread it on tin sheets and heat them with a steam coil. The tannin quickly puffs up and dries.
Outils nécessaires :
Tôle de fer-blanc
Serpentin de vapeur
Chaudière à vapeur
Gants en caoutchoucMatériaux
1- 1 as requiredEspace réservé
Outils requis
16- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
- Espace réservé
Ce plan fabrique
Blueprints liés
Ces blueprints partagent des connaissances — techniques, matériaux ou principes
CC0 Domaine public
Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.
Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.