Guitar Strings: Bronze Wound on Steel, Then Heat-Soaked (Stone and Falcone 1977)
Woody

Créé par

Woody

28. octobre 2026NO
3
0
0
0
0

Guitar Strings: Bronze Wound on Steel, Then Heat-Soaked (Stone and Falcone 1977)

A wound string is a steel core with another wire wrapped round it. Stone and Falcone believed the wrap keeps stresses from the winding and slowly unwinds as the string is played, so the tone goes dead. Their fix: after winding, heat-soak the string, at least 2 hours at 270 °F or 30 minutes at 480 °F for a bronze wrap, then let it cool. Source: W. N. Stone and A. S. Falcone (National Musical String Co.), US 4,063,674 (1977). Unknown: the winding itself (the patent calls it conventional), where phosphor bronze wire comes from, and the gauges. These are linked to unknown heads. The plain strings of the set are steel music wire; that, the oven and the nitrogen are ours. Picture drawn by Youblob.
Avancé
1 day

Consignes

1

Cut the core and plain strings

Cut steel music wire for the cores of the wound strings and for the plain strings of the set. Unknown: the gauges and lengths, and the ball ends.

Matériaux pour cette étape :

Corde à piano en acier 0,032"Corde à piano en acier 0,032"1 as required

Outils nécessaires :

Pince coupantePince coupante
Dimensions inconnuesDimensions inconnues
2

Wind the bronze wrap at room temperature

Wrap phosphor bronze wire helically round each core at room temperature. The patent prefers a wrap that expands more with heat than the core. Unknown: how; the patent says only 'in a conventional manner'.

Matériaux pour cette étape :

Fil de bronze phosphoreuxFil de bronze phosphoreux1 as required

Outils nécessaires :

Méthode de filage inconnueMéthode de filage inconnue
Dimensions inconnuesDimensions inconnues
Lunettes de sécuritéLunettes de sécurité
3

Heat-soak the wound strings

Heat the wound strings for a bronze wrap at 270-480 °F (132-249 °C): at least 2 hours at 270 °F or at least 30 minutes at 480 °F, shorter the hotter. If the wire tarnishes in hot air, do it without air, in nitrogen or carbon dioxide. The wrap's turns settle into more even spacing.

Outils nécessaires :

FourFour
Thermomètre de laboratoireThermomètre de laboratoire
Bouteille d’azoteBouteille d’azote
4

Cool and set up the set

Let the strings cool back to room temperature. Make up the set with the plain steel strings.

Outils nécessaires :

Pince coupantePince coupante

Matériaux

2

Outils requis

7

CC0 Domaine public

Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.

Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.

Commentaires

(0)

Se connecter pour participer à la discussion

Chargement des commentaires...