Crucible Furnace: the Brass Founder's Sunk Coke Air Furnace (Larkin, 1907)
The brass founder's crucible furnace: a firebrick-lined pit sunk below the floor, fired with hard coke on an iron grating over the ash-pit, closed by a dome-shaped iron cover and drawn by a flue with a damper. The crucible sits on a firebrick in the middle of the fire, lidded, with coke banked round it, until the metal is melted.
Result: a coke-fired crucible furnace for melting brass and bronze.
Source: J. Larkin, The Practical Brass and Iron Founder's Guide (1907), pp. 96-99. Unknown: all sizes. Picture drawn by Youblob.
Menengah
Unknown
Instruksi
1
1
Build the pit
Build the pit
Sink the furnace below the floor. Line the inside with firebricks set in fireclay; use pure clay (white, opaque, oily to the touch), since iron oxide, magnesia, lime or black lead in brick or clay shortens the furnace's life. Close the ash-pit at the bottom with a hinged iron grating. Not given: sizes.
Material untuk langkah ini:
Bata Tahan Api1 lining
Tanah Liat Tahan Api1 jointing
Logam tidak diketahui1 hinged gratingAlat yang dibutuhkan:
Dimensi tidak diketahui2
2
Fit the cover and flue
Fit the cover and flue
Make a dome-shaped cover for the furnace top of cast or wrought iron. Lead a flue from the furnace with a damper in it. Not given: the flue size or height.
Material untuk langkah ini:
Logam tidak diketahui1 dome cover, damper
Pipa cerobong asap1 flueAlat yang dibutuhkan:
Dimensi tidak diketahui3
3
Fire it and melt
Fire it and melt
Burn hard coke broken to lumps the size of a fist. Heat the crucible bottom upwards in the fire, lift it out with the tongs, turn it upright and bed it on a slab of fireclay or a firebrick, put on its lid and bank the fire round it. Put the metal in, close the cover and open the damper for draught until the metal is melted. Black-lead crucibles last longer; clay ones must first be hardened by slowly raising their temperature.
Alat yang dibutuhkan:
Kokas metalurgi
Kowi grafit-lempung
Penjepit KowiBahan
4- 1 liningPlaceholder
- 1 jointingPlaceholder
- 1 dome cover, damperPlaceholder
- 1 fluePlaceholder
Alat yang Diperlukan
4- Placeholder
- Placeholder
- Placeholder
- Placeholder
Bahan cetak biru terhubung
Cetak biru ini membuat