Crude Naphthalene from Light Creosote Oil: Warnes, 1913
Charlie

Dibuat oleh

Charlie

13. Oktober 2026DE
16
0
0
0
0

Crude Naphthalene from Light Creosote Oil: Warnes, 1913

How a coal-tar works made crude naphthalene, from Arthur R. Warnes's Coal Tar Distillation (1913). The naphthalene crystallises out of the light creosote oil (middle or carbolic oil) as it stands. It is melted, recrystallised and drained, sold as drained naphthalene, or pressed hard in bags as pressed naphthalene.
Lanjutan
Works process

Instruksi

1

Salt out the oil

Use washed light creosote, quite free from tarry matter. Pump it into crystallising boilers and let it stand for several days, on average 3 to 5 depending on the time of year, while the naphthalene, the "salts", crystallises out. Then drain the separated oil away through the drain pipes.

Material untuk langkah ini:

Minyak kreosot ringanMinyak kreosot ringan1 as required

Alat yang dibutuhkan:

Tangki kristalisasiTangki kristalisasi
Pompa pemindahPompa pemindah
2

Melt and recrystallise

Melt the crude naphthalene left in the boilers with closed steam. When it is all liquid and well above its crystallising point, pump it into the recrystallising tanks, and at once blow steam through the pipes so no liquid salts set solid in them. Let it cool and recrystallise from the oil carried over.

Alat yang dibutuhkan:

Ketel uapKetel uap
Pompa pemindahPompa pemindah
Tangki kristalisasiTangki kristalisasi
TermometerTermometer
3

Drain it

After two to four days open the drain taps and run off the oil that has separated. When the crude naphthalene has thoroughly drained, it can be packed in barrels as drained naphthalene.

Alat yang dibutuhkan:

Tangki kristalisasiTangki kristalisasi
Tong kayuTong kayu
4

Press it in bags

For pressed naphthalene, fill press bags (sometimes ordinary sacking) with the recrystallised crude, about 9 by 18 by 3 inches, keeping them evenly thick. Lay them on the press table about 2 inches apart, cover with a wrought-iron plate about 1/4 inch thick, and build up layer on layer, each lying squarely over the one below. Raise the press gently, then slowly increase the pressure to 1 1/2 to 2 tons per square inch and hold about an hour.

Alat yang dibutuhkan:

Mesin pres hidrolikMesin pres hidrolik
Pelat besiPelat besi
Karung goniKarung goni
5

Trim and break up the cakes

Release the pressure and take the cakes from the bags. Cut off any wet edges and press them again with the next batch. Break the cakes up in a disintegrator and pack them.

Alat yang dibutuhkan:

PisauPisau
Mesin penghancurMesin penghancur
6

The press load

Memuat notebook Jupyter…

Bahan

1

Alat yang Diperlukan

10

Cetak biru ini membuat

Blueprint terkait

Blueprint ini berbagi pengetahuan — teknik, bahan, atau prinsip

CC0 Domain Publik

Cetak biru ini dirilis di bawah CC0. Anda bebas untuk menyalin, memodifikasi, mendistribusikan, dan menggunakan karya ini untuk tujuan apa pun, termasuk komersial, tanpa meminta izin.

Dukung Maker dengan membeli produk melalui Cetak Biru mereka di mana mereka mendapatkan Komisi Pembuat yang ditetapkan oleh Penjual, atau buat iterasi baru dari Cetak Biru ini dan masukkan sebagai koneksi di milik Anda sendiri.

Diskusi

(0)

Masuk untuk bergabung dengan diskusi

Memuat komentar...