Wire Enamel: Polyvinyl Formal and Cresol Resin in Solvent, Jackson and Hall 1938

GE's 1938 magnet-wire enamel: 10.67 % polyvinyl formal and 5.33 % cresol-formaldehyde resin dissolved in cresol and a hydrocarbon solvent, stirred until clear and viscous, then filtered. Wire drawn through it and baked at 250–500 °C, several passes, gets a tough, flexible insulation. We use benzene, one of the solvents the patent allows. The picture: our diagram of the mixing.
Lanjutan
A few hours

Konten berbahaya

Blueprint ini mengandung prosedur berbahaya. Masuk dan aktifkan konten berbahaya di pengaturan akun Anda untuk melihat petunjuk langkah demi langkah.

Masuk

CC0 Domain Publik

Cetak biru ini dirilis di bawah CC0. Anda bebas untuk menyalin, memodifikasi, mendistribusikan, dan menggunakan karya ini untuk tujuan apa pun, termasuk komersial, tanpa meminta izin.

Dukung Maker dengan membeli produk melalui Cetak Biru mereka di mana mereka mendapatkan Komisi Pembuat yang ditetapkan oleh Penjual, atau buat iterasi baru dari Cetak Biru ini dan masukkan sebagai koneksi di milik Anda sendiri.

Diskusi

(0)

Masuk untuk bergabung dengan diskusi

Memuat komentar...