Iron Axle and Cams for a Trip Hammer, Forged from Wrought Iron
A trip hammer is raised by a cam and drops under its own weight. The cams are lugs on a revolving shaft turned by the water wheel; each one lifts the helve once a turn. Forge a wrought-iron axle with a squared middle and three curved cams that slide on and are wedged tight.
The picture: our diagram, side and end view.
Lanjutan
Three days with a striker
Instruksi
1
1
Weld up the axle
Weld up the axle
Bind wrought-iron bars into a faggot as long as the shaft, bring it to a welding heat, sprinkle with sand and weld it solid with a striker, a heat at a time along its length.
Material untuk langkah ini:
Batang besi tempa25 kg
Tongkat besi tempa1 mAlat yang dibutuhkan:
Perapian pandai besi
Arang
Pasir Halus
Godam
Palu pandai besi
Tang pandai besi
Landasan Tempa
Sarung tangan las
Kacamata pengaman
Celemek Kulit2
2
Shape the axle
Shape the axle
Leave the middle square for the cams and draw both ends round for the journals. Flatter the square true and file the journals smooth.
Alat yang dibutuhkan:
Perapian pandai besi
Perata tempa
Godam
Tang pandai besi
Landasan Tempa
Kikir Logam
Sarung tangan las
Kacamata pengaman
Celemek Kulit3
3
Forge the cams
Forge the cams
For each cam, forge a thick curved lug on a boss. Punch the boss and drift it square to slide over the axle's square.
Material untuk langkah ini:
Batang besi tempa6 kgAlat yang dibutuhkan:
Perapian pandai besi
Pelubang panas
Pelebar lubang tirus
Pahat potong landasan
Godam
Palu pandai besi
Tang pandai besi
Landasan Tempa
Sarung tangan las
Kacamata pengaman
Celemek Kulit4
4
Fit and wedge
Fit and wedge
Slide the three cams onto the square at equal turns round the shaft, each lined up with the helve's tail. Drive iron wedges beside each boss until tight.
Material untuk langkah ini:
Tongkat besi tempa0.5 mAlat yang dibutuhkan:
Palu pandai besi
Kikir Logam
Landasan Tempa
Sarung tangan las
Kacamata pengaman
Celemek Kulit5
5
Blows per minute
Blows per minute
Memuat notebook Jupyter…
Bahan
2- 25 kgPlaceholder
- Placeholder
Alat yang Diperlukan
15- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
- Placeholder
Cetak biru ini membuat
Blueprint terkait
Blueprint ini berbagi pengetahuan — teknik, bahan, atau prinsip
CC0 Domain Publik
Cetak biru ini dirilis di bawah CC0. Anda bebas untuk menyalin, memodifikasi, mendistribusikan, dan menggunakan karya ini untuk tujuan apa pun, termasuk komersial, tanpa meminta izin.
Dukung Maker dengan membeli produk melalui Cetak Biru mereka di mana mereka mendapatkan Komisi Pembuat yang ditetapkan oleh Penjual, atau buat iterasi baru dari Cetak Biru ini dan masukkan sebagai koneksi di milik Anda sendiri.