Empty Paint Tube: Soldered Sheet Lead, Rand 1841

John Rand's 1841 patent names grain-tin, lead and pewter for paint tubes. The metal only has to be thin enough to yield to pressure and stay collapsed. His own tube was drawn tin about 1/75 inch thick, but he writes that a tube of sheet metal with a soldered seam works as well. This is that route in lead: roll a strip round a former, solder the seam, close one end, and leave the other open for filling. Source: J. Rand, US 2,252 (1841). The sheet thickness, former, flux, size and tools are ours. The picture is the patent's drawing sheet.
متوسط
1 hour

دستورالعمل‌ها

1

Cut the strip

Cut a strip of thin lead sheet as long as the tube and wide enough to go once round the former with a narrow overlap. Rand asks only for metal thin enough to yield to pressure and stay collapsed; ours is Ure's thinner cast sheet, 1/48 in (0.5 mm). Longer tubes need somewhat thicker metal.

مواد مورد نیاز این مرحله:

ورق سربورق سرب1 as required

ابزارهای مورد نیاز:

قیچی ورق‌بریقیچی ورق‌بری
خط‌کشخط‌کش
2

Roll it round a former

Roll the strip round a round wooden dowel so the edges overlap, and press the seam flat. The dowel and the overlap are ours.

ابزارهای مورد نیاز:

گل‌میخ چوبیگل‌میخ چوبی
3

Solder the seam

Join the edges by soldering, one of the two ways Rand gives (the other is melting the edges together). Ours: a little rosin flux and tin-lead solder run along the seam with a hot iron, on the dowel. Slide the tube off.

مواد مورد نیاز این مرحله:

لحیم قلع-سربلحیم قلع-سرب1 as required
خمیر روان‌ساز لحیم (بر پایهٔ کلوفن)خمیر روان‌ساز لحیم (بر پایهٔ کلوفن)1 as required

ابزارهای مورد نیاز:

هویههویه
گل‌میخ چوبیگل‌میخ چوبی
4

Close one end

Press the edges of one end together with flat pliers (Rand used forceps that leave a groove along the end). Close it by adding a little solder with a hot iron. Leave the other end open: the tube is filled from there and then closed the same way.

مواد مورد نیاز این مرحله:

لحیم قلع-سربلحیم قلع-سرب1 as required

ابزارهای مورد نیاز:

انبردست تختانبردست تخت
هویههویه

مواد

3

ابزارهای لازم

5
  • جایگزین
  • جایگزین
  • جایگزین
  • 2 vendors sell this, none ship to you yet
    جایگزین
  • جایگزین

نقشه‌های مرتبط

این نقشه‌ها دانش مشترکی دارند — تکنیک‌ها، مواد یا اصول

CC0 مالکیت عمومی

این نقشه تحت مجوز CC0 منتشر شده است. شما آزاد هستید آن را کپی، ویرایش، توزیع و برای هر هدفی بدون نیاز به اجازه استفاده کنید.

با خرید محصولات از طریق نقشه از سازنده حمایت کنید و او کمیسیون سازنده تعیین شده توسط فروشندگان، دریافت می‌کند یا یک نسخه جدید از این نقشه ایجاد کنید و آن را به عنوان اتصال در نقشه خود قرار دهید تا درآمد به اشتراک گذاشته شود.

بحث و گفتگو

(0)

ورود برای شرکت در بحث

در حال بارگذاری نظرات...