Tsvet's Column: The First Chromatogram

In 1903 a Russian-Italian botanist working in Warsaw poured an extract of green leaves into a glass tube packed with powdered chalk, washed it through with petroleum solvent, and watched the single green smear pull apart into separate coloured bands down the column. Mikhail Tsvet called the result a *chromatogram* — a writing in colour — and it is the ancestor of every separation in this batch. His insight was that leaf green is not one substance: it is two chlorophylls and a family of yellow and orange carotenoids, and they stick to chalk with different strengths. The one that clings least travels furthest. The technique was ignored for thirty years, partly because Tsvet published in Russian and partly because the leading plant chemist of the day insisted the bands were artefacts. You can settle that argument yourself in an afternoon with chalk and a glass tube.
متوسط
4 hours

دستورالعمل‌ها

1

Get the pigments out of the leaf

Grind a handful of fresh spinach in a mortar with a little clean sand and enough ethanol to make a slurry, then filter. You want a dark green extract, not a pale one. The sand is doing real work: it tears the cell walls and the chloroplast membranes open so the solvent can reach pigments that are otherwise locked inside. Grinding without it gives a weak extract and a column with nothing to show. Keep the extract in the dark — chlorophyll bleaches in light, and a sunlit extract loses its top band before you have packed the tube.

مواد مورد نیاز این مرحله:

اسفناجاسفناج100 گرم
اتانول - درجهٔ آزمایشگاهی، 95 %اتانول - درجهٔ آزمایشگاهی، 95 %50 میلی‌لیتر
ماسهٔ کوارتزماسهٔ کوارتز20 گرم

ابزارهای مورد نیاز:

هاون و دستهٔ هاونهاون و دستهٔ هاون
قیف شیشه‌ای پایه‌دارقیف شیشه‌ای پایه‌دار
کاغذ صافیکاغذ صافی
بشر بوروسیلیکاتبشر بوروسیلیکات
2

Pack the column evenly, or it will run crooked

Plug the bottom of a glass tube with a small wad of cotton wool, add a centimetre of sand, then pour in powdered chalk a little at a time, tapping the side constantly, to a depth of about 15 cm. Finish with another centimetre of sand on top. Tapping is not fussiness. Any gap or crack in the packing becomes a channel the solvent races down, and the bands come out slanted, smeared or merged. The sand layers protect the chalk surface from being cratered when you pour, which does the same damage in a different way.

مواد مورد نیاز این مرحله:

کربنات کلسیم (گرد سفیدآب)کربنات کلسیم (گرد سفیدآب)100 گرم
ماسهٔ کوارتزماسهٔ کوارتز30 گرم
پنبهٔ جاذبپنبهٔ جاذب1 بسته

ابزارهای مورد نیاز:

میله شیشه بوروسیلیکاتمیله شیشه بوروسیلیکات
3

Wet the column before you load it — never let it run dry

Run solvent through until the whole packing is wetted and a few millimetres stand above the top sand. Keep it that way for the rest of the run. A column that runs dry cracks, and a cracked column is finished — you cannot re-wet it back into a uniform bed. This is the single rule that decides whether the afternoon works. Set the solvent reservoir up so it keeps the level topped up rather than trusting yourself to notice.

مواد مورد نیاز این مرحله:

استوناستون100 میلی‌لیتر

ابزارهای مورد نیاز:

بشر بوروسیلیکاتبشر بوروسیلیکات
4

Load a narrow band, and let it sink in

Let the solvent drain to exactly the top of the sand, then pipette your extract gently down the inside wall so it forms a thin, level layer. Let THAT drain in before adding any solvent. The width of the band you start with is the width you are stuck with. Every separation that follows has to pull the components further apart than this starting smear, so a 2 mm load separates where a 2 cm load never will. This is the same discipline as a narrow spot in paper chromatography, and it matters more here because the column is longer.

ابزارهای مورد نیاز:

پیپت مدرّج (مور)پیپت مدرّج (مور)
5

Develop, and watch the green come apart

Add solvent steadily and let it run. Over twenty minutes or so the single green band stretches, then splits: a yellow-orange band running ahead, then yellow-green, then blue-green behind. Ahead are the carotenes, which barely stick to the chalk. Behind them the xanthophylls, which carry oxygen atoms and hold on harder. Last come chlorophyll a and then chlorophyll b, the most strongly held of all. You are watching a mixture sort itself by how tightly each molecule grips a surface — and this is exactly the argument Tsvet lost for thirty years.

مواد مورد نیاز این مرحله:

استوناستون200 میلی‌لیتر

ابزارهای مورد نیاز:

بشر بوروسیلیکاتبشر بوروسیلیکات
6

Collect the bands as separate fractions

Put a fresh test tube under the outlet as each coloured band approaches, and change tubes as it passes. Cap and label each one. This is the step that turns a pretty demonstration into chemistry. A band you watched is a picture; a band in a tube is a purified substance you can weigh, spectroscope, or run again. Tsvet's own word for the separated bands was 'zones', and collecting them is what earned the method its place when Kuhn and Lederer rediscovered it in the 1930s.

ابزارهای مورد نیاز:

لولهٔ آزمایش (بوروسیلیکات)لولهٔ آزمایش (بوروسیلیکات)
پیپت مدرّج (مور)پیپت مدرّج (مور)
7

Why the bands travel at different speeds

در حال بارگذاری دفترچهٔ Jupyter…

ابزارهای مورد نیاز:

خط‌کشخط‌کش
8

Change the solvent and watch the order hold

Run the column again with a solvent of different polarity — swap some of the acetone for a less polar solvent, or the reverse — and note what changes. The bands move faster or slower, sometimes dramatically, but their ORDER stays the same, because the order is set by how strongly each pigment grips the chalk relative to the others. Solvent strength is your speed control; the stationary phase decides the sequence. Understanding which knob does which is the difference between tuning a separation and guessing at one.

مواد مورد نیاز این مرحله:

ایزوپروپیل الکل ۹۹ ٪ایزوپروپیل الکل ۹۹ ٪100 میلی‌لیتر
استوناستون100 میلی‌لیتر

ابزارهای مورد نیاز:

بشر بوروسیلیکاتبشر بوروسیلیکات

مواد

7

ابزارهای لازم

8

CC0 مالکیت عمومی

این نقشه تحت مجوز CC0 منتشر شده است. شما آزاد هستید آن را کپی، ویرایش، توزیع و برای هر هدفی بدون نیاز به اجازه استفاده کنید.

با خرید محصولات از طریق نقشه از سازنده حمایت کنید و او کمیسیون سازنده تعیین شده توسط فروشندگان، دریافت می‌کند یا یک نسخه جدید از این نقشه ایجاد کنید و آن را به عنوان اتصال در نقشه خود قرار دهید تا درآمد به اشتراک گذاشته شود.

بحث و گفتگو

(0)

ورود برای شرکت در بحث

در حال بارگذاری نظرات...