Annealing Oven: a Firebrick Chamber over a Firebox
Bubbles

Búin til af

Bubbles

14. október 2026IT
14
0
0
0
0

Annealing Oven: a Firebrick Chamber over a Firebox

Annealing is holding work hot and letting it cool slowly so it loses its stresses or softens. Glass is held at about 454–482 °C for most kinds, then cooled slowly; metal is often left to cool in the oven with the fire out. Build a firebrick chamber over a small firebox, with a door, a damper and a pyrometer, so it can be held at heat and then shut up to cool. The picture: putting bottles into the annealing oven at a glass works, 1908 (Lewis Hine).
Miðlungs
Two days, then drying

Leiðbeiningar

1

Lay the firebox

On a level base, lay firebricks in refractory mortar for a small firebox with an opening for fuel and air.

Efni fyrir þetta skref:

Eldfastur steinnEldfastur steinn40 stykki
Eldfast leirmúrEldfast leirmúr10 kg

Nauðsynleg verkfæri:

MúrskeiðMúrskeið
HallamálHallamál
2

Grate and chamber

Forge iron bars to lay across the top of the firebox as a floor with gaps for the heat, and build the chamber walls on it, leaving a flue hole in the roof.

Efni fyrir þetta skref:

SmíðajárnsstöngSmíðajárnsstöng4 stykki
Eldfastur steinnEldfastur steinn30 stykki
Eldfast leirmúrEldfast leirmúr10 kg

Nauðsynleg verkfæri:

SmiðjueldstæðiSmiðjueldstæði
SteðjiSteðji
ÞverfleygshamarÞverfleygshamar
MúrskeiðMúrskeið
3

Door, damper and pyrometer

Fit an iron-sheet door lined with brick and a sliding sheet damper over the flue. Set the pyrometer through the side wall into the chamber.

Efni fyrir þetta skref:

Járnplata (hömruð)Járnplata (hömruð)2 stykki

Nauðsynleg verkfæri:

ÞverfleygshamarÞverfleygshamar
HáhitamælirHáhitamælir
4

Dry and first firing

Let the mortar dry for several days, then fire gently with charcoal and raise the heat slowly. Practise holding the chamber at the heat you need, and shutting door, damper and firebox to cool it down slowly.

Efni fyrir þetta skref:

ViðarkolViðarkol10 as required

Nauðsynleg verkfæri:

HáhitamælirHáhitamælir
Hitaþolnir hanskarHitaþolnir hanskar
5

Bricks for the oven

Hleð Jupyter-vinnubók…

Efni

5

Nauðsynleg verkfæri

7

Tengd Blueprint

Þessi blueprint deila þekkingu — tækni, efni eða meginreglur

CC0 opinbert ríki

Þessi teikning er gefin út undir CC0. Þér er frjálst að afrita, breyta, dreifa og nota þetta verk í hvaða tilgangi sem er, án þess að biðja um leyfi.

Studdu smiðinn með því að kaupa vörur í gegnum teikningu hans þar sem hann fær þóknun smiða sem seljendur ákvarða, eða búðu til nýja endurskoðun á þessari teikningu og tengdu hana sem tengingu í þinni eigin teikningu til að deila tekjum.

Umræða

(0)

Skrá inn til að taka þátt í umræðunni

Hleður athugasemdum...