Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1300 °C, 1.0 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1300 °C, 1.0 mm (Masuyama 1972)

eftir EdFI

Iðnaður

5
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1150 °C, 1.0 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1150 °C, 1.0 mm (Masuyama 1972)

eftir EdFI

Iðnaður

3
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 800 °C, 1.0 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 800 °C, 1.0 mm (Masuyama 1972)

eftir EdFI

Iðnaður

1
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 750 °C, 1.0 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 750 °C, 1.0 mm (Masuyama 1972)

eftir EdFI

Iðnaður

5
0
0
0
0
0
Extruded Polystyrene Foam: Butylene-Blown Logs 20 Inches Across (McIntire, Dow 1948, Ex. 4)

Extruded Polystyrene Foam: Butylene-Blown Logs 20 Inches Across (McIntire, Dow 1948, Ex. 4)

eftir CharlieDE

Lífrænt

10
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 75 °C (McIntire, Dow 1948, Ex. 3, Test 4)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 75 °C (McIntire, Dow 1948, Ex. 3, Test 4)

eftir CharlieDE

Lífrænt

10
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 60 °C (McIntire, Dow 1948, Ex. 3, Test 3)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 60 °C (McIntire, Dow 1948, Ex. 3, Test 3)

eftir CharlieDE

Lífrænt

11
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 50 °C (McIntire, Dow 1948, Ex. 3, Test 2)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 50 °C (McIntire, Dow 1948, Ex. 3, Test 2)

eftir CharlieDE

Lífrænt

12
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 40 °C (McIntire, Dow 1948, Ex. 3, Test 1)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 40 °C (McIntire, Dow 1948, Ex. 3, Test 1)

eftir CharlieDE

Industry 3.0 — Assembly Line & Mass Production (1913)

10
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 100 °C (McIntire, Dow 1948, Ex. 2)
Hættulegt

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 100 °C (McIntire, Dow 1948, Ex. 2)

eftir CharlieDE

Lífrænt

15
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)
Hættulegt

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)

eftir CharlieDE

Lífrænt

13
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 80 °C (McIntire, Dow 1948, Ex. 2)
Hættulegt

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 80 °C (McIntire, Dow 1948, Ex. 2)

eftir CharlieDE

Lífrænt

15
0
0
0
0
0
Dichloromethane: Chloroform Reduced with Zinc, Alcohol and Hydrochloric Acid (Greene, in Thorpe 1912)
Hættulegt

Dichloromethane: Chloroform Reduced with Zinc, Alcohol and Hydrochloric Acid (Greene, in Thorpe 1912)

eftir CharlieDE

Lífrænt

15
0
0
0
0
0
Strontium Ferrite Disc Magnet: Example 9 Without the Orienting Field (Gorter, Philips 1956, Ex. 9 Comparison)

Strontium Ferrite Disc Magnet: Example 9 Without the Orienting Field (Gorter, Philips 1956, Ex. 9 Comparison)

eftir CharlieDE

Efni

14
0
0
0
0
0
Oriented Strontium Ferrite Disc Magnet: Less Iron Oxide, 10,000 Oersted Field (Gorter, Philips 1956, Ex. 9)

Oriented Strontium Ferrite Disc Magnet: Less Iron Oxide, 10,000 Oersted Field (Gorter, Philips 1956, Ex. 9)

eftir CharlieDE

Efni

8
0
0
0
0
0
Strontium Ferrite Disc Magnet: Example 8 Without the Orienting Field (Gorter, Philips 1956, Ex. 8 Comparison)

Strontium Ferrite Disc Magnet: Example 8 Without the Orienting Field (Gorter, Philips 1956, Ex. 8 Comparison)

eftir CharlieDE

Efni

8
0
0
0
0
0
Oriented Strontium Ferrite Disc Magnet: Agate-Milled, 10,000 Oersted Field (Gorter, Philips 1956, Ex. 8)

Oriented Strontium Ferrite Disc Magnet: Agate-Milled, 10,000 Oersted Field (Gorter, Philips 1956, Ex. 8)

eftir CharlieDE

Efni

9
0
0
0
0
0
Barium Ferrite Disc Magnet: Example 7 Without the Orienting Field (Gorter, Philips 1956, Ex. 7 Comparison)

Barium Ferrite Disc Magnet: Example 7 Without the Orienting Field (Gorter, Philips 1956, Ex. 7 Comparison)

eftir CharlieDE

Efni

12
0
0
0
0
0
Oriented Barium Ferrite Disc Magnet: Powder Ground 48 Hours (Gorter, Philips 1956, Ex. 7)

Oriented Barium Ferrite Disc Magnet: Powder Ground 48 Hours (Gorter, Philips 1956, Ex. 7)

eftir CharlieDE

Efni

13
0
0
0
0
0
Oriented Barium Ferrite Disc Magnet: Heated to 500 °C Without a Field (Gorter, Philips 1956, Ex. 6)

Oriented Barium Ferrite Disc Magnet: Heated to 500 °C Without a Field (Gorter, Philips 1956, Ex. 6)

eftir CharlieDE

Efni

14
0
0
0
0
0
Oriented Barium Ferrite Disc Magnet: Water Instead of a Binder (Gorter, Philips 1956, Ex. 5)

Oriented Barium Ferrite Disc Magnet: Water Instead of a Binder (Gorter, Philips 1956, Ex. 5)

eftir CharlieDE

Efni

9
0
0
0
0
0
Barium Ferrite Disc Magnet: Example 4 Without the Orienting Field (Gorter, Philips 1956, Ex. 4 Comparison)

Barium Ferrite Disc Magnet: Example 4 Without the Orienting Field (Gorter, Philips 1956, Ex. 4 Comparison)

eftir CharlieDE

Efni

12
0
0
0
0
0
Oriented Barium Ferrite Disc Magnet: 10,000 Oersted Field (Gorter, Philips 1956, Ex. 4)

Oriented Barium Ferrite Disc Magnet: 10,000 Oersted Field (Gorter, Philips 1956, Ex. 4)

eftir CharlieDE

Efni

13
0
0
0
0
0
Oriented Barium Ferrite Disc Magnet: Binder Dried in a 2400 Oersted Field (Gorter, Philips 1956, Ex. 3)

Oriented Barium Ferrite Disc Magnet: Binder Dried in a 2400 Oersted Field (Gorter, Philips 1956, Ex. 3)

eftir CharlieDE

Efni

8
0
0
0
0
0