Carbon Film Resistors: Methane Cracked on Ceramic Rods, Helixed and Varnished (Bell Labs 1951)
Ed

Búin til af

Ed

2. nóvember 2026FI
6
0
0
0
0

Carbon Film Resistors: Methane Cracked on Ceramic Rods, Helixed and Varnished (Bell Labs 1951)

Ceramic rods tumble in a hot, gas-tight rotating furnace while methane cracks on them and leaves a thin, hard film of carbon. The coated rods get conducting ends, a helix ground through the film to bring them near their value, a light rub to the exact value, and a coat of baking varnish. Result: carbon film resistors adjusted to as close as ±0.5 %. The helix alone can raise a rod's resistance by any factor from about 10 to about 8000. Source: Grisdale, Pfister and van Roosbroeck, Pyrolytic Film Resistors, Bell System Technical Journal 30 (1951). Unknown: the ceramic of the rods, the end caps and leads, and which baking varnish; the paper does not give them. Picture: Wikimedia Commons.
Lengra kominn
2 days

Leiðbeiningar

1

Load the furnace

Load cylindrical ceramic rods into the gas-tight refractory core of a rotating (or rocking) batch furnace, with silica sand to support the rods and keep them from damage as they tumble. Unknown: which ceramic.

Efni fyrir þetta skref:

Einangrandi viðnámskjarniEinangrandi viðnámskjarni1 batch

Nauðsynleg verkfæri:

SnúningslotuofnSnúningslotuofn
KvarssandurKvarssandur
2

Heat under nitrogen

Turn the core and bring it to temperature, usually about 975 to 1300 °C, flushing it with nitrogen before any hydrocarbon goes in.

Nauðsynleg verkfæri:

SnúningslotuofnSnúningslotuofn
KöfnunarefniKöfnunarefni
3

Crack the methane

When the temperature is steady, let in the coating gas and keep it flowing for the time needed. The film grows at a steady rate: at 1000 °C and 30 % methane the paper runs from 0.2 to 10 hours. Longer gives a thicker film of lower resistance; temperature sets the rate more than anything else, and more methane deposits faster.

Efni fyrir þetta skref:

MetanMetan1 flow

Nauðsynleg verkfæri:

SnúningslotuofnSnúningslotuofn
4

Cool under nitrogen

Shut off the methane and let the core cool while oxygen-free nitrogen keeps flowing. The films come out clean, even and firmly stuck.

Nauðsynleg verkfæri:

SnúningslotuofnSnúningslotuofn
KöfnunarefniKöfnunarefni
5

Terminate the ends

Paint the ends of each coated rod with a water suspension of colloidal graphite (Aquadag), then burnish and bake it; this suits all but low-value resistors. Fit the end caps with their leads. Unknown: the caps and leads, which the paper does not describe. Ours: an agate burnisher and an oven.

Efni fyrir þetta skref:

KvoðugrafítKvoðugrafít1 as required
Endahettur viðnáms með leiðslumEndahettur viðnáms með leiðslum2 per resistor

Nauðsynleg verkfæri:

AgatgljáirAgatgljáir
BakarofnBakarofn
6

Grind the helix

Grind a helical groove through the film with a water-cooled, metal-bonded diamond wheel, the blank floating against the wheel so the groove stays even. Pick the pitch to land slightly below the wanted value (330 Ω, 10 kΩ or any other). The groove must be smooth: cracks into the carbon ribbon bring noise and drift.

Nauðsynleg verkfæri:

Gormskurðarvél fyrir viðnámGormskurðarvél fyrir viðnám
7

Rub to value and varnish

Turn the resistor while measuring it continuously, and rub its whole surface lightly with a cotton pad wet with an organic solvent until it reaches its value. Leave it just below tolerance, then give it one or more coats of baking varnish, which raises the resistance by generally less than 1 %. Unknown: which varnish and its baking. Ours: acetone as the solvent, a Wheatstone bridge to measure.

Efni fyrir þetta skref:

OfnlakkOfnlakk1 as required

Nauðsynleg verkfæri:

Wheatstone-brúWheatstone-brú
HreinsibómullHreinsibómull
AsetónAsetón
BakarofnBakarofn

Efni

5

Nauðsynleg verkfæri

9

Tengd Blueprint

Þessi blueprint deila þekkingu — tækni, efni eða meginreglur

CC0 opinbert ríki

Þessi teikning er gefin út undir CC0. Þér er frjálst að afrita, breyta, dreifa og nota þetta verk í hvaða tilgangi sem er, án þess að biðja um leyfi.

Studdu smiðinn með því að kaupa vörur í gegnum teikningu hans þar sem hann fær þóknun smiða sem seljendur ákvarða, eða búðu til nýja endurskoðun á þessari teikningu og tengdu hana sem tengingu í þinni eigin teikningu til að deila tekjum.

Umræða

(0)

Skrá inn til að taka þátt í umræðunni

Hleður athugasemdum...