Wire Enamel: Polyvinyl Formal and Cresol Resin in Solvent, Jackson and Hall 1938
GE's 1938 magnet-wire enamel: 10.67 % polyvinyl formal and 5.33 % cresol-formaldehyde resin dissolved in cresol and a hydrocarbon solvent, stirred until clear and viscous, then filtered. Wire drawn through it and baked at 250–500 °C, several passes, gets a tough, flexible insulation. We use benzene, one of the solvents the patent allows.
The picture: our diagram of the mixing.
Lengra kominn
A few hours
Hættulegt efni
Þessi teikning inniheldur hættulegar aðferðir. Skráðu þig inn og virkjaðu hættulegt efni í stillingum reikningsins til að sjá skref-fyrir-skref leiðbeiningar.
Skrá innÞessi teikning býr til
Tengd Blueprint
Þessi blueprint deila þekkingu — tækni, efni eða meginreglur

Hættulegt
Polyvinyl Formal: Polyvinyl Acetate Acetalised with Formalin, Shawinigan 1933
eftir Charlie
Fjölliða
4
0
0
0
0
0

Hættulegt
Cresol-Formaldehyde Resin for Wire Enamel, Jackson and Hall 1938
eftir Charlie
Fjölliða
3
0
0
0
0
0

Hættulegt
Benzene from Coal-Tar Light Oil: Washed and Rectified, Lunge 1887
eftir Charlie
Iðnaður
1
0
0
0
0
0
CC0 opinbert ríki
Þessi teikning er gefin út undir CC0. Þér er frjálst að afrita, breyta, dreifa og nota þetta verk í hvaða tilgangi sem er, án þess að biðja um leyfi.
Studdu smiðinn með því að kaupa vörur í gegnum teikningu hans þar sem hann fær þóknun smiða sem seljendur ákvarða, eða búðu til nýja endurskoðun á þessari teikningu og tengdu hana sem tengingu í þinni eigin teikningu til að deila tekjum.