Glass Tube: Drawn by Two Glassmakers Walking Apart (Pellatt, 1849)
Charlie

Búin til af

Charlie

4. nóvember 2026DE
5
0
0
2
0

Glass Tube: Drawn by Two Glassmakers Walking Apart (Pellatt, 1849)

How glass tube was made by hand: a blown gather of glass is welded at one end to a second rod, and two workers walk away from each other while turning, stretching the hot glass into a tube up to 60 or 70 feet long. Because the whole bubble stretches evenly, the bore and the wall stay in the same proportion all along the tube. Result: long glass tube of nearly even bore, cut into lengths when cold. Solid cane is made the same way without blowing. Source: Apsley Pellatt, Curiosities of Glass Making (1849), pp. 106-108. Unknown: the glass batch and the gather's size. Picture: the book's figures.
Sérfræðingur
Unknown

Leiðbeiningar

1

Gather and blow the ball

Gather a solid ball of flint glass on the end of the blowing iron and blow it out a little, so it is hollow. When it has partly cooled, use it as a core for one or more further gatherings until there is enough glass. For flat-bore thermometer tube, flatten the first ball on the marver with an iron or wooden battledore before the later gatherings. Ours: lead crystal. Not given: the amount of glass.

Efni fyrir þetta skref:

BlýkristallBlýkristall1 flint glass

Nauðsynleg verkfæri:

Glerofn sem nær 1100 gráðum á CelsíusGlerofn sem nær 1100 gráðum á Celsíus
GlerblásturspípaGlerblásturspípa
Marver (völsunarplata glerblásarans)Marver (völsunarplata glerblásarans)
2

Swing it long and fix the post

Lengthen the ball by swinging it, and chill its far end by dipping it in cold water. A second worker makes a disc of hot glass on a rod, the 'post', and holds it upright near the ground. The chief worker climbs onto a chair and drops the hot ball onto the post, where it welds on.

Nauðsynleg verkfæri:

VatnVatn
PontustöngPontustöng
3

Walk apart and draw

The chief worker steps down and the two walk away from each other, both turning their rods all the time. At first the hot glass sags between them in a curve; fan the parts that are thicker to cool them, so it stretches evenly. Draw it to the length wanted, up to 60 or 70 feet; as it cools it stops turning and pulls nearly straight. Except at the ends, it has nearly one bore, diameter and wall thickness. Ours: a wooden paddle for fanning (Pellatt: a boy's hat).

Nauðsynleg verkfæri:

GlerblásturspípaGlerblásturspípa
PontustöngPontustöng
TréspaðiTréspaði
4

Lay down and cut

Lay the tube across the wooden rungs of a ladder to cool. Cut it into lengths by touching it with a cold iron or nicking it with a steel file.

Nauðsynleg verkfæri:

TréstigiTréstigi
MálmþjölMálmþjöl

Efni

1
  • 1 flint glass
    Staðgengill

Nauðsynleg verkfæri

8

Þessi teikning býr til

CC0 opinbert ríki

Þessi teikning er gefin út undir CC0. Þér er frjálst að afrita, breyta, dreifa og nota þetta verk í hvaða tilgangi sem er, án þess að biðja um leyfi.

Studdu smiðinn með því að kaupa vörur í gegnum teikningu hans þar sem hann fær þóknun smiða sem seljendur ákvarða, eða búðu til nýja endurskoðun á þessari teikningu og tengdu hana sem tengingu í þinni eigin teikningu til að deila tekjum.