Guitar Strings: Bronze Wound on Steel, Then Heat-Soaked (Stone and Falcone 1977)

A wound string is a steel core with another wire wrapped round it. Stone and Falcone believed the wrap keeps stresses from the winding and slowly unwinds as the string is played, so the tone goes dead. Their fix: after winding, heat-soak the string, at least 2 hours at 270 °F or 30 minutes at 480 °F for a bronze wrap, then let it cool. Source: W. N. Stone and A. S. Falcone (National Musical String Co.), US 4,063,674 (1977). Unknown: the winding itself (the patent calls it conventional), where phosphor bronze wire comes from, and the gauges. These are linked to unknown heads. The plain strings of the set are steel music wire; that, the oven and the nitrogen are ours. Picture drawn by Youblob.
Lengra kominn
1 day

Leiðbeiningar

1

Cut the core and plain strings

Cut steel music wire for the cores of the wound strings and for the plain strings of the set. Unknown: the gauges and lengths, and the ball ends.

Efni fyrir þetta skref:

Fjaðurstálsvír 0,032 tommurFjaðurstálsvír 0,032 tommur1 as required

Nauðsynleg verkfæri:

HliðarbíturHliðarbítur
Óþekkt málÓþekkt mál
2

Wind the bronze wrap at room temperature

Wrap phosphor bronze wire helically round each core at room temperature. The patent prefers a wrap that expands more with heat than the core. Unknown: how; the patent says only 'in a conventional manner'.

Efni fyrir þetta skref:

FosfórbronsvírFosfórbronsvír1 as required

Nauðsynleg verkfæri:

Óþekkt vafningsaðferðÓþekkt vafningsaðferð
Óþekkt málÓþekkt mál
ÖryggisglerauguÖryggisgleraugu
3

Heat-soak the wound strings

Heat the wound strings for a bronze wrap at 270-480 °F (132-249 °C): at least 2 hours at 270 °F or at least 30 minutes at 480 °F, shorter the hotter. If the wire tarnishes in hot air, do it without air, in nitrogen or carbon dioxide. The wrap's turns settle into more even spacing.

Nauðsynleg verkfæri:

BakarofnBakarofn
RannsóknastofuhitamælirRannsóknastofuhitamælir
KöfnunarefnishylkiKöfnunarefnishylki
4

Cool and set up the set

Let the strings cool back to room temperature. Make up the set with the plain steel strings.

Nauðsynleg verkfæri:

HliðarbíturHliðarbítur

Efni

2

Nauðsynleg verkfæri

7

CC0 opinbert ríki

Þessi teikning er gefin út undir CC0. Þér er frjálst að afrita, breyta, dreifa og nota þetta verk í hvaða tilgangi sem er, án þess að biðja um leyfi.

Studdu smiðinn með því að kaupa vörur í gegnum teikningu hans þar sem hann fær þóknun smiða sem seljendur ákvarða, eða búðu til nýja endurskoðun á þessari teikningu og tengdu hana sem tengingu í þinni eigin teikningu til að deila tekjum.

Umræða

(0)

Skrá inn til að taka þátt í umræðunni

Hleður athugasemdum...