Annealing Oven: a Firebrick Chamber over a Firebox
Bubbles

Creato da

Bubbles

14. ottobre 2026IT
13
0
0
0
0

Annealing Oven: a Firebrick Chamber over a Firebox

Annealing is holding work hot and letting it cool slowly so it loses its stresses or softens. Glass is held at about 454–482 °C for most kinds, then cooled slowly; metal is often left to cool in the oven with the fire out. Build a firebrick chamber over a small firebox, with a door, a damper and a pyrometer, so it can be held at heat and then shut up to cool. The picture: putting bottles into the annealing oven at a glass works, 1908 (Lewis Hine).
Intermedio
Two days, then drying

Istruzioni

1

Lay the firebox

On a level base, lay firebricks in refractory mortar for a small firebox with an opening for fuel and air.

Materiali per questo passaggio:

Mattoni refrattariMattoni refrattari40 pezzi
Malta di argilla refrattariaMalta di argilla refrattaria10 kg

Strumenti necessari:

Cazzuola da muratoreCazzuola da muratore
Livella a bollaLivella a bolla
2

Grate and chamber

Forge iron bars to lay across the top of the firebox as a floor with gaps for the heat, and build the chamber walls on it, leaving a flue hole in the roof.

Materiali per questo passaggio:

Barra di ferro battutoBarra di ferro battuto4 pezzi
Mattoni refrattariMattoni refrattari30 pezzi
Malta di argilla refrattariaMalta di argilla refrattaria10 kg

Strumenti necessari:

Forgia da fabbroForgia da fabbro
IncudineIncudine
Martello a penna trasversaleMartello a penna trasversale
Cazzuola da muratoreCazzuola da muratore
3

Door, damper and pyrometer

Fit an iron-sheet door lined with brick and a sliding sheet damper over the flue. Set the pyrometer through the side wall into the chamber.

Materiali per questo passaggio:

Lamiera di ferro (battuta)Lamiera di ferro (battuta)2 pezzi

Strumenti necessari:

Martello a penna trasversaleMartello a penna trasversale
PirometroPirometro
4

Dry and first firing

Let the mortar dry for several days, then fire gently with charcoal and raise the heat slowly. Practise holding the chamber at the heat you need, and shutting door, damper and firebox to cool it down slowly.

Materiali per questo passaggio:

Carbone di legnaCarbone di legna10 as required

Strumenti necessari:

PirometroPirometro
Guanti resistenti al caloreGuanti resistenti al calore
5

Bricks for the oven

Caricamento del notebook Jupyter…

Materiali

5

Strumenti richiesti

7

Blueprint correlati

Questi blueprint condividono conoscenze — tecniche, materiali o principi

CC0 Pubblico dominio

Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.

Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.

Commenti

(0)

Accedi per partecipare alla discussione

Caricamento commenti...