Bearing Steel Bar (52100): Crucible Steel Alloyed with Chromium

52100 is the steel of ball bearings: about 1 % carbon and 1.5 % chromium (ASM). The standard, ASTM A295, allows 0.93–1.05 % carbon and 1.35–1.60 % chromium. Here crucible steel is melted with chromium and a little manganese, cast, forged to bar and annealed soft for working. Our method, not the factory one: factory 52100 is melted in an electric furnace and vacuum-degassed to meet the standard's limits on inclusions. A crucible melt can reach the composition, but only a lab test shows whether it is clean enough for bearings. The picture: our drawing, crucible to bar.
Avanzato
2 days

Istruzioni

1

Weigh the charge

For 1 kg: 981.5 g crucible steel of about 1 % carbon, 15 g chromium and 3.5 g manganese (our figures; see the last step). Use steel whose analysis you know.

Materiali per questo passaggio:

Acciaio al crogioloAcciaio al crogiolo981.5 g
Cromo metallicoCromo metallico15 g
ManganeseManganese3.5 g

Strumenti necessari:

Bilancia digitale da cucinaBilancia digitale da cucina
2

Melt

Pack the steel, chromium and manganese in a covered clay crucible and melt it in the furnace. The alloy is fully liquid above 1450 °C.

Strumenti necessari:

Crogiolo di argilla profondoCrogiolo di argilla profondo
Forno in mattoniForno in mattoni
ManticeMantice
Guanti da saldatoreGuanti da saldatore
Grembiule di cuoioGrembiule di cuoio
Occhiali di sicurezzaOcchiali di sicurezza
3

Cast the ingot

Lift the crucible out with tongs and pour into a cast-iron ingot mould. Let it cool.

Strumenti necessari:

Tenaglia per crogioloTenaglia per crogiolo
LingottieraLingottiera
Guanti da saldatoreGuanti da saldatore
Grembiule di cuoioGrembiule di cuoio
Occhiali di sicurezzaOcchiali di sicurezza
4

Forge to bar

Heat the ingot to a cherry-red heat and no hotter, and draw it out on the anvil to a round or square bar. Reheat when the colour drops; never hammer it cold.

Materiali per questo passaggio:

Carbone di legnaCarbone di legna1 as required

Strumenti necessari:

Forgia da fabbroForgia da fabbro
IncudineIncudine
MazzaMazza
Martello a penna trasversaleMartello a penna trasversale
Tenaglie da fabbroTenaglie da fabbro
Calibro digitale da 6 polliciCalibro digitale da 6 pollici
Guanti da saldatoreGuanti da saldatore
Grembiule di cuoioGrembiule di cuoio
Occhiali di sicurezzaOcchiali di sicurezza
5

Test the analysis

Drill clean chips from the bar and have a lab analyse carbon, chromium, manganese, silicon, phosphorus and sulphur. Keep the bar only if it is within 52100 limits.

Strumenti necessari:

Trapano a manoTrapano a mano
Barattoli di vetro con coperchioBarattoli di vetro con coperchio
Occhiali di sicurezzaOcchiali di sicurezza
6

Anneal soft

In the oven, hold the bar at 793 °C (1460 °F) for 30 minutes, cool in the oven no faster than 500 °C an hour to 682 °C (1260 °F), then cool in air (Verhoeven's anneal).

Strumenti necessari:

Forno per trattamenti termiciForno per trattamenti termici
Termocoppia con lettoreTermocoppia con lettore
Tenaglie da fabbroTenaglie da fabbro
Guanti da saldatoreGuanti da saldatore
7

The charge

Caricamento del notebook Jupyter…

Materiali

4

Strumenti richiesti

19

CC0 Pubblico dominio

Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.

Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.

Commenti

(0)

Accedi per partecipare alla discussione

Caricamento commenti...