Crucible Furnace: the Brass Founder's Sunk Coke Air Furnace (Larkin, 1907)

The brass founder's crucible furnace: a firebrick-lined pit sunk below the floor, fired with hard coke on an iron grating over the ash-pit, closed by a dome-shaped iron cover and drawn by a flue with a damper. The crucible sits on a firebrick in the middle of the fire, lidded, with coke banked round it, until the metal is melted. Result: a coke-fired crucible furnace for melting brass and bronze. Source: J. Larkin, The Practical Brass and Iron Founder's Guide (1907), pp. 96-99. Unknown: all sizes. Picture drawn by Youblob.
Intermedio
Unknown

Istruzioni

1

Build the pit

Sink the furnace below the floor. Line the inside with firebricks set in fireclay; use pure clay (white, opaque, oily to the touch), since iron oxide, magnesia, lime or black lead in brick or clay shortens the furnace's life. Close the ash-pit at the bottom with a hinged iron grating. Not given: sizes.

Materiali per questo passaggio:

Mattoni refrattariMattoni refrattari1 lining
Argilla refrattariaArgilla refrattaria1 jointing
Metallo sconosciutoMetallo sconosciuto1 hinged grating

Strumenti necessari:

Dimensioni sconosciuteDimensioni sconosciute
2

Fit the cover and flue

Make a dome-shaped cover for the furnace top of cast or wrought iron. Lead a flue from the furnace with a damper in it. Not given: the flue size or height.

Materiali per questo passaggio:

Metallo sconosciutoMetallo sconosciuto1 dome cover, damper
Tubo fumarioTubo fumario1 flue

Strumenti necessari:

Dimensioni sconosciuteDimensioni sconosciute
3

Fire it and melt

Burn hard coke broken to lumps the size of a fist. Heat the crucible bottom upwards in the fire, lift it out with the tongs, turn it upright and bed it on a slab of fireclay or a firebrick, put on its lid and bank the fire round it. Put the metal in, close the cover and open the damper for draught until the metal is melted. Black-lead crucibles last longer; clay ones must first be hardened by slowly raising their temperature.

Strumenti necessari:

Coke metallurgicoCoke metallurgico
Crogiolo grafite-argillaCrogiolo grafite-argilla
Tenaglia per crogioloTenaglia per crogiolo

Materiali

4

Strumenti richiesti

4

Questo progetto realizza

CC0 Pubblico dominio

Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.

Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.

Commenti

(0)

Accedi per partecipare alla discussione

Caricamento commenti...