LDPE Pellets: Ethylene Polymerised at 1500 Atmospheres with a Trace of Oxygen

Polyethylene was discovered at ICI by Fawcett, Gibson and Perrin (US 2,153,553, 1939): ethylene squeezed to over a thousand atmospheres and heated, with a trace of oxygen to start the reaction, turns into a tough, waxy solid that melts at about 120 °C. Their Example III, at 1500 atmospheres and 210 °C for 5 hours, turned 80 % of the ethylene into polymer. The heat of reaction must be carried away, or the gas decomposes explosively. Extruding it into pellets is our step. The picture: our diagram.
Avanzato
About 6 hours

Contenuto pericoloso

Questo blueprint contiene procedure pericolose. Accedi e abilita i contenuti pericolosi nelle impostazioni del tuo account per visualizzare le istruzioni passo dopo passo.

Accedi

Questo progetto realizza

Blueprint correlati

Questi blueprint condividono conoscenze — tecniche, materiali o principi

CC0 Pubblico dominio

Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.

Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.

Commenti

(0)

Accedi per partecipare alla discussione

Caricamento commenti...