Oxalic Acid: Wood Soaked in Caustic Alkali and Heated in Hot Air at 300 °C (Plater-Syberg)
Pericoloso
Charlie

Creato da

Charlie

21. ottobre 2026DE
0
0
0
0
0

Oxalic Acid: Wood Soaked in Caustic Alkali and Heated in Hot Air at 300 °C (Plater-Syberg)

Oxalic acid from wood by Plater-Syberg's process (English Patent 23682, 1893), as Thorpe's Dictionary (1913) gives it: wood soaked in caustic alkali is heated in hot air. At about 120 °C it gives mostly acetic acid; at about 300 °C with more air, almost only oxalate. The oxalate is turned into calcium oxalate, which sulphuric acid breaks up to oxalic acid. Hot caustic and strong acid burn: goggles, gloves. The picture: our diagram.
Avanzato
3 days

Contenuto pericoloso

Questo blueprint contiene procedure pericolose. Accedi e abilita i contenuti pericolosi nelle impostazioni del tuo account per visualizzare le istruzioni passo dopo passo.

Accedi

CC0 Pubblico dominio

Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.

Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.

Commenti

(0)

Accedi per partecipare alla discussione

Caricamento commenti...