Technical Molybdic Oxide: Molybdenite Roasted in Nichols-Herreshoff Furnaces (US Bureau of Mines 1957)
Molybdenite concentrate is roasted in air in a multiple-hearth furnace: it dries on the top hearth at 300 °F and roasts on the lower hearths at up to 1,250 °F, coming out about 4 hours later as molybdic oxide.
Result: technical molybdic oxide with 0.06 to 0.30 % sulphur, packed in cans or bags for the steel industry.
Source: US Bureau of Mines Information Circular 7784, Molybdenum - A Materials Survey (1957), p. 37, practice of Molybdenum Corporation of America at Washington, Pa. Not given: feed rate, air, fuel, yield. The sulphur leaves as sulphur dioxide, a poisonous gas. Picture drawn by Youblob.
Avanzato
4 hours
Contenuto pericoloso
Questo blueprint contiene procedure pericolose. Accedi e abilita i contenuti pericolosi nelle impostazioni del tuo account per visualizzare le istruzioni passo dopo passo.
AccediQuesto progetto realizza
CC0 Pubblico dominio
Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.
Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.