Wire Cutters: Diagonal Pliers Forged with Hardened V-Edged Jaws
Diagonal pliers cut wire by pressing two V-shaped edges into it until it splits, not by shearing like scissors. The edges sit at an angle to the joint rivet, which gives them their name, and the jaws must be hardened or steel wire dents them. Forge two halves from tool steel, rivet them, grind the edges and harden the jaws.
The picture: the jaws and joint of a modern pair; its handles are dipped in plastic, ours are bare steel.
Avanzato
Two days
Istruzioni
1
1
Forge the halves
Forge the halves
Forge two mirror halves from tool steel: a short, thick jaw set at an angle, a flat boss for the joint, and a handle (our sizes: jaw 18 mm, handle 120 mm from the joint).
Materiali per questo passaggio:
Barra ottagonale di acciaio per utensili0.3 kg
Carbone di legna2 as requiredStrumenti necessari:
Forgia da fabbro
Incudine
Martello a penna trasversale
Tenaglie da fabbro
Guanti da saldatore
Occhiali di sicurezza2
2
Anneal and fit the joint
Anneal and fit the joint
Anneal both halves. File the bosses flat so they lap closely, drill them together and rivet them so the jaws close without play.
Materiali per questo passaggio:
Rivetti in acciaio1 pezzoStrumenti necessari:
Forgia da fabbro
Lima per metalli
Trapano a mano
Morsa da banco pesante
Martello a penna trasversale
Incudine3
3
Grind the edges
Grind the edges
Grind each jaw to a symmetrical V so the two edges meet along their whole length when closed. Check against the light.
Strumenti necessari:
Mola ad acqua
Lima per metalli4
4
Harden the jaws
Harden the jaws
Heat the jaws only to cherry red and quench in water. Polish them bright, then warm the joint and let the colour run to the edges; quench at straw (our temper).
Materiali per questo passaggio:
Acqua10 litriStrumenti necessari:
Forgia da fabbro
Tinozza di tempra
Tenaglie da fabbro
Guanti da saldatore
Occhiali di sicurezza5
5
Hone and test
Hone and test
Hone the edges lightly on the stone and try them on soft copper wire first. A dent in the edge means the jaw is too soft.
Strumenti necessari:
Pietra per affilare grana 10006
6
Force at the edges
Force at the edges
Caricamento del notebook Jupyter…
Materiali
4- Segnaposto
- 2 as requiredSegnaposto
- 1 pezzoSegnaposto
- 10 litriSegnaposto
Strumenti richiesti
12- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
- Segnaposto
Questo progetto realizza
Blueprint correlati
Questi blueprint condividono conoscenze — tecniche, materiali o principi
CC0 Pubblico dominio
Questo progetto è rilasciato sotto CC0. Sei libero di copiare, modificare, distribuire e utilizzare quest'opera per qualsiasi scopo, senza chiedere permesso.
Supporta il Maker acquistando prodotti tramite il suo progetto dove guadagna una Commissione Maker stabilita dai venditori, oppure crea una nuova iterazione di questo progetto e includilo come collegamento nel tuo progetto per condividere i ricavi.