Electrolytic Capacitors: Borate Paper Wound with Formed Aluminium Foil and Vacuum-Impregnated (Danziger, US 2,107,780)
Ed

作成者

Ed

2. 11月 2026FI
7
0
0
0
0

Electrolytic Capacitors: Borate Paper Wound with Formed Aluminium Foil and Vacuum-Impregnated (Danziger, US 2,107,780)

A dry electrolytic capacitor wound from aluminium foil and paper. The paper is first soaked in ammonium borate and dried, so the salt is already in its fibres. After winding, the bodies are soaked under heat and vacuum in borate dissolved in glycol, boxed and aged at 500 volts. Result: electrolytic capacitors. In the patent's tests these lost only 4.8 % of their capacity, against about 33 % for bodies made the ordinary way, and their power-factor loss rose 87 % on life test against 250 %. Source: H. I. Danziger and A. Di Giacomo, US 2,107,780 (1938). Unknown: how the anode foil is formed, which paper, the tab metal, and how the ammonium borate is made; the patent does not give them. Picture: Wikimedia Commons.
上級者
1 day

手順

1

Salt the paper

Draw the paper strip through a saturated solution of ammonium borate in water, about 15 to 30 seconds for each part of it, then dry it at about 80 °C for about 15 seconds and reel it up. The salted paper keeps until needed. Unknown: which paper. Ours: a tray for the bath and a drying oven.

このステップの材料:

コンデンサ用セパレータ紙コンデンサ用セパレータ紙1 strip
ホウ酸アンモニウムホウ酸アンモニウム1 to saturate

必要な工具:

水水
トレートレー
乾燥炉乾燥炉
2

Wind the bodies

On a winding machine, wind two aluminium foil strips with the salted paper between them onto a mandrel; at least one foil must already carry its electrolytic film. One paper strip is enough. Let the paper stand out at both ends, bring a connection tab out of each end, cut the strips and hold the body wound with a rubber band. Unknown: how the foil was formed, and the tab metal.

このステップの材料:

化成アルミ箔化成アルミ箔1 strip
アルミ箔アルミ箔1 strip
不明な金属不明な金属2 tabs

必要な工具:

コンデンサ巻取機コンデンサ巻取機
輪ゴム輪ゴム
3

Make the impregnant

Heat ethylene glycol to about 90 °C, then stir in powdered ammonium borate slowly and continuously until the solution reaches about 122 °C. Ours: a hot plate and thermometer.

このステップの材料:

エチレングリコールエチレングリコール1 as required
ホウ酸アンモニウムホウ酸アンモニウム1 as required

必要な工具:

ホットプレートホットプレート
温度計温度計
4

Soak under heat and vacuum

Rack the bodies in a vacuum tank heated to about 50 °C and draw about 745 mm of vacuum for about an hour to pull out air and moisture. Draw in the impregnant at about 85 °C, ease the vacuum to about 310 mm, and hold at about 85 °C for about another hour.

必要な工具:

蒸気ジャケット付き真空容器蒸気ジャケット付き真空容器
真空ポンプ真空ポンプ
温度計温度計
5

Box and age

Take the bodies out, put them in cardboard containers, and age them at about 500 volts DC for about three hours.

このステップの材料:

紙管紙管1 per capacitor

必要な工具:

高電圧直流電源(卓上)高電圧直流電源(卓上)

材料

7

必要な工具

10

関連ブループリント

これらのブループリントは知識を共有しています — 技術、材料、原理

CC0 パブリックドメイン

このブループリントはCC0で公開されています。許可を求めずに、自由にコピー、修正、配布、あらゆる目的で使用できます。

メイカーを応援するには、ブループリント経由で製品を購入してください。メイカーには メイカーコミッション がベンダーにより設定されています。または、このブループリントの新しいイテレーションを作成し、自分のブループリントにコネクションとして含めて収益を共有できます。

ディスカッション

(0)

ログイン してディスカッションに参加

コメントを読み込み中...