Plastic Extruder: Steam-Jacketed Screw Stuffer with a Heated Nozzle (Andersen & Strasdin, US 2,384,521, 1945)
Emma

作成者

Emma

3. 11月 2026SE
8
0
0
0
0

Plastic Extruder: Steam-Jacketed Screw Stuffer with a Heated Nozzle (Andersen & Strasdin, US 2,384,521, 1945)

A screw extruder for thermoplastics: a turning screw in a steam-jacketed barrel pushes hot, softened plastic forward through a short nozzle heated electrically. The barrel is kept a little below the plastic's flow temperature and the nozzle well above it, so the extruded rod comes out with a smooth, glass-like skin. Result: an extruder that makes rod, tube or strip at 25 to 30 feet a minute. Source: B. Andersen and R. F. Strasdin (Celanese), US 2,384,521 (1945). Unknown: sizes and metals. Picture: the patent drawing.
上級者
Unknown

手順

1

Make the screw

Turn a screw to fit the barrel. Its thread may be single or double; to press the plastic harder toward the nozzle, make the pitch increase or the groove get shallower toward that end. Example: a double-thread screw. Ours: mild steel. Not given: sizes.

このステップの材料:

軟鋼丸棒軟鋼丸棒1 screw

必要な工具:

金属旋盤金属旋盤
フライス盤フライス盤
不明な寸法不明な寸法
2

Make the jacketed barrel

Make the barrel with a steam jacket round it and a steam port into the jacket, and a feed throat at the back end. The inside wall may be grooved, pitched so that every flight of the screw always meets a groove; this stops the plastic slipping. Not given: the metal, the steam pressure.

このステップの材料:

不明な金属不明な金属1 barrel and jacket

必要な工具:

金属旋盤金属旋盤
不明な寸法不明な寸法
3

Fit the heated nozzle

At the front, fit a streamlined nozzle head so no plastic can pocket and decompose, and a nozzle 1/2 to 18 inches long; about 6 inches in the example. Perforated plates may go between the screw and the nozzle. Heat the nozzle with an electric resistance coil. Ours: nichrome wire.

このステップの材料:

不明な金属不明な金属1 nozzle head and nozzle
ニクロム線ニクロム線1 nozzle heating coil
不明な絶縁材料不明な絶縁材料1 coil insulation

必要な工具:

金属旋盤金属旋盤
4

Drive the screw

Drive the screw through a gear from a motor, so its speed can be kept steady; 20 revolutions a minute in the example. Not given: the drive.

このステップの材料:

電動機電動機1 drive motor
不明な金属不明な金属1 drive gears

必要な工具:

不明な寸法不明な寸法
5

Extrude a rod

Keep the barrel 0 to 100 °F below the plastic's flow temperature and the nozzle 50 to 100 °F above it. Example: barrel at about 270 °F by steam, nozzle at about 400 °F, for a cellulose acetate with a flow temperature of 307 °F. Feed the hot, softened plastic into the throat at a steady rate. Carry the rod away on a conveyor and cool it at once with cold water, then cut it to length.

必要な工具:

蒸気ボイラー蒸気ボイラー
高温計高温計
水水

材料

5
  • プレースホルダー
  • 1 drive gears
    プレースホルダー
  • 1 nozzle heating coil
    プレースホルダー
  • 1 coil insulation
    プレースホルダー
  • 1 drive motor
    プレースホルダー

必要な工具

6

CC0 パブリックドメイン

このブループリントはCC0で公開されています。許可を求めずに、自由にコピー、修正、配布、あらゆる目的で使用できます。

メイカーを応援するには、ブループリント経由で製品を購入してください。メイカーには メイカーコミッション がベンダーにより設定されています。または、このブループリントの新しいイテレーションを作成し、自分のブループリントにコネクションとして含めて収益を共有できます。

ディスカッション

(0)

ログイン してディスカッションに参加

コメントを読み込み中...