Calcined Copper Concentrate: Pyritic Concentrates Roasted to 8 % Sulphur in Allen-O'Harra Calciners (Butte, Peters 1905)
Hatari
Charlie

Imeundwa na

Charlie

1. Novemba 2026DE
4
0
0
0
0

Calcined Copper Concentrate: Pyritic Concentrates Roasted to 8 % Sulphur in Allen-O'Harra Calciners (Butte, Peters 1905)

Pyritic copper concentrates carry about 40 % sulphur, far too much to smelt to a rich matte. At Butte they were dragged along two 90 ft hearths by chain-drawn ploughs while wood fires burned part of the sulphur away. Result: calcines with 8 to 9 % sulphur, 50 tons a day from each furnace; the concentrates lose 26 % of their dry weight. Source: Edward D. Peters, Modern Copper Smelting (1905), pp. 201-204; picture: his Plate II, the Allen-O'Harra calciner. Not given: temperature, time on the hearths. Roasting gives off sulphur dioxide, a poisonous gas.
Juu
1 day

Maudhui hatari

Blueprint hii ina taratibu za hatari. Ingia na uwashe maudhui ya hatari katika mipangilio ya akaunti yako ili kuona maagizo ya hatua kwa hatua.

Ingia

CC0 Umma Wote

Mchoro huu umetolewa chini ya CC0. Uko huru kunakili, kubadilisha, kusambaza, na kutumia kazi hii kwa madhumuni yoyote, bila kuomba ruhusa.

Saidia Mtengenezaji kwa kununua bidhaa kupitia Mchoro wao ambapo wanapata Kamisheni ya Mtengenezaji iliyowekwa na Wachuuzi, au unda marudio mapya ya Mchoro huu na uiunganishe kama kiungo katika Mchoro wako kuchangia mapato.

Majadiliano

(0)

Ingia kujiunga na majadiliano

Inapakia maoni...