A flat screwdriver is a steel shank flattened to a blade that fits the slot of a screw. H. Holford's 20th Century Toolsmith and Steelworker (1907) says most smiths make them so they twist or break on a hard screw, and gives his cure: forge it from 75-point carbon steel, strike the blade a few good blows on each flat at a low heat, harden it and let the temper run to grey. His Fig. 60 shows the shape without its handle. He gives no sizes and no handle, which are unknown here; the brine bath is from his chapter on the hardening bath. Source: H. Holford (1907), pp. 21, 118. Picture: his Fig. 60.
Kati
Half a day

Maagizo

1

Read Holford

"Strike it a few good blows on each flat side of the screw driving edge while at a low heat. Then harden and allow the temper to draw to a grey, cool off and you will have a screw driver that will give unlimited satisfaction."
2

Forge the shape

Take good steel of 75 points carbon. Forge it to the shape of Fig. 60: a round shank, flattened at one end to the driving blade and drawn to a pointed tang at the other for the handle. Holford gives no sizes (unknown).

Vifaa kwa hatua hii:

Kipande cha mraba cha feleji ya zanaKipande cha mraba cha feleji ya zana1 bar

Zana zinazohitajika:

Jiko la KufuaJiko la Kufua
FuaweFuawe
Nyundo ya mhunziNyundo ya mhunzi
Koleo za mhunziKoleo za mhunzi
Vipimo visivyojulikanaVipimo visivyojulikana
Miwani ya usalamaMiwani ya usalama
Glavu Zinazostahimili JotoGlavu Zinazostahimili Joto
3

Pack the blade

At a low heat, strike a few good blows on each flat side of the driving edge.

Zana zinazohitajika:

Nyundo ya mhunziNyundo ya mhunzi
FuaweFuawe
Jiko la KufuaJiko la Kufua
Koleo za mhunziKoleo za mhunzi
4

Harden and temper grey

Heat the blade end evenly and quench it in the hardening bath. Holford's bath is clean water free from grease, best made into a brine with as much salt as the water will dissolve, kept as large and as cold as possible. Brighten the blade with a file so the colours show, draw the temper to a grey, then cool it off.

Zana zinazohitajika:

Jiko la KufuaJiko la Kufua
Myeyusho wa chumvi uliojaaMyeyusho wa chumvi uliojaa
Koleo za mhunziKoleo za mhunzi
Tupa lainiTupa laini
Glavu Zinazostahimili JotoGlavu Zinazostahimili Joto
5

Fit a handle

Fit a handle on the tang. Holford shows the screwdriver without one and does not say what it is made of (unknown).

Vifaa kwa hatua hii:

Nyenzo isiyojulikanaNyenzo isiyojulikana1 handle
6

History and honest limits

Holford, a toolsmith writing for blacksmiths and tool dressers, says a good screwdriver is prized by every mechanic, woodworkers most of all, yet few smiths could make one that would not break or twist. His temper table lists the screwdriver at grey, in 0.75 carbon steel. He gives no sizes, no handle and no heat for hardening; those are unknown here, and the tools are ours.

Vifaa

2

Zana Zinazohitajika

9

Blueprint zinazohusiana

Blueprint hizi zinashiriki maarifa — mbinu, vifaa au kanuni

CC0 Umma Wote

Mchoro huu umetolewa chini ya CC0. Uko huru kunakili, kubadilisha, kusambaza, na kutumia kazi hii kwa madhumuni yoyote, bila kuomba ruhusa.

Saidia Mtengenezaji kwa kununua bidhaa kupitia Mchoro wao ambapo wanapata Kamisheni ya Mtengenezaji iliyowekwa na Wachuuzi, au unda marudio mapya ya Mchoro huu na uiunganishe kama kiungo katika Mchoro wako kuchangia mapato.

Majadiliano

(0)

Ingia kujiunga na majadiliano

Inapakia maoni...