Wash and Rub Fastness: Testing the Colour Before You Trust It
Tex

Imeundwa na

Tex

24. Septemba 2026FO
21
0
0
0
0

Wash and Rub Fastness: Testing the Colour Before You Trust It

A freshly dyed skein always looks good. The question is what it looks like after a winter of wear and half a dozen washes, and that is answered by testing rather than by hoping. Three different things are meant by "fastness" and a dye can be good at one and bad at another. **Wash fastness** is whether the colour stays in the fibre in hot soapy water. **Rub fastness**, or crocking, is whether it comes off on a hand or another garment. **Light fastness** is whether it survives daylight, and has its own blueprint. All three can be tested at home in a way that is honest, and the tests take minutes.
Kati
3 hours

Maagizo

1

The wash test, and the white witness beside it

Cut two small pieces of the dyed fibre. Keep one as the control, somewhere dark. Take the other and pin a piece of undyed white cotton or wool against it. Wash both together in water at 40 C with a little neutral detergent, worked gently for half an hour, then rinse and dry them flat. Then read two things: **The sample against the control.** How much paler has it gone? A little is normal; a lot means dye that was never bonded. **The white witness.** How much colour has moved onto it? This is the number that matters for a garment, because it is what will happen to everything else in the wash. The witness is the part beginners leave out, and it is the half that predicts the disaster. A skein can hold its own depth perfectly and still ruin a load of washing.

Vifaa kwa hatua hii:

Uzi wa sufu usiotiwa rangiUzi wa sufu usiotiwa rangi1 shada
Kitambaa cha pamba (chepesi)Kitambaa cha pamba (chepesi)1 m
Sabuni lainiSabuni laini1 kipande

Zana zinazohitajika:

Mitungi ya kioo yenye vifunikoMitungi ya kioo yenye vifuniko
MkasiMkasi
Kadi za faharasaKadi za faharasa
Kichanja cha KukaushiaKichanja cha Kukaushia
2

The rub test takes ten seconds

Rub a piece of dry white cotton firmly against the dyed fibre, ten strokes, always in the same direction. Then wet a second piece and do the same again. Look at both white pieces. Any colour on them is colour that will come off on skin, on a shirt collar, on a chair. The wet test is nearly always worse than the dry one, which is why it is worth doing both. **Indigo is the famous case.** Indigo is held mechanically in the fibre rather than bonded to it, so even a well-made indigo crocks — and that is exactly what produces the worn highlights on old denim. It is a property of the dye, not a fault in the work, and it can be reduced but not removed by thorough rinsing and by not building the depth too fast. **Heavy shades crock more than pale ones**, in every dye, because there is more surface dye sitting on top of what actually bonded.

Vifaa kwa hatua hii:

Kitambaa cha pamba (chepesi)Kitambaa cha pamba (chepesi)1 m
Uzi wa sufu usiotiwa rangiUzi wa sufu usiotiwa rangi1 shada

Zana zinazohitajika:

MkasiMkasi
Kadi za faharasaKadi za faharasa
3

Scoring it so the answer means something next year

A note saying "faded a bit" is worth nothing six months later. Use a scale and keep the samples. The textile industry uses a five-point grey scale where 5 is no change and 1 is severe change. A home dyer can use the same five points honestly by keeping the control alongside: **5** — no difference visible against the control. **4** — a difference only visible when they are held touching. **3** — clearly different, still obviously the same colour. **2** — strongly changed. **1** — a different colour. Score the sample and the white witness separately; they are different numbers. Staple both pieces and the control to the record card. The stapled scrap is the measurement — anything written down is a description of it.

Vifaa kwa hatua hii:

Uzi wa sufu usiotiwa rangiUzi wa sufu usiotiwa rangi1 shada

Zana zinazohitajika:

Kadi za faharasaKadi za faharasa
MkasiMkasi
4

What to do about a poor result

Poor fastness has a small number of causes and most of them are fixable next time. **Overloaded bath.** More dye was used than the fibre could bond, so the excess sits on the surface. Symptom: rinse water that never runs clear, heavy crocking, big loss in the first wash. Use less dye, or ladder a second skein through it. **Under-mordanted.** Especially cellulose without a tannin step. Symptom: pale result and most of it washes out. **Struck too fast.** Hot entry, so the dye grabbed the surface instead of penetrating. Symptom: uneven as well as unfast. **Not rinsed properly.** Symptom: colour in the first wash and then nothing much afterwards. This is the cheapest one to fix, and a proper rinse — until the water runs clear, at bath temperature — is part of the dyeing, not the tidying up. For an existing skein that crocks, more rinsing genuinely helps. A wash in warm water with a little detergent removes surface dye and the skein ends slightly paler and much better behaved. Do that before it is knitted, not after.

Vifaa kwa hatua hii:

Uzi wa sufu usiotiwa rangiUzi wa sufu usiotiwa rangi2 shada
Sabuni lainiSabuni laini1 kipande

Zana zinazohitajika:

Chungu kikubwaChungu kikubwa
KipimajotoKipimajoto
Kichanja cha KukaushiaKichanja cha Kukaushia
Kadi za faharasaKadi za faharasa

Vifaa

3

Zana Zinazohitajika

6

CC0 Umma Wote

Mchoro huu umetolewa chini ya CC0. Uko huru kunakili, kubadilisha, kusambaza, na kutumia kazi hii kwa madhumuni yoyote, bila kuomba ruhusa.

Saidia Mtengenezaji kwa kununua bidhaa kupitia Mchoro wao ambapo wanapata Kamisheni ya Mtengenezaji iliyowekwa na Wachuuzi, au unda marudio mapya ya Mchoro huu na uiunganishe kama kiungo katika Mchoro wako kuchangia mapato.

Majadiliano

(0)

Ingia kujiunga na majadiliano

Inapakia maoni...