Bone Ash by Calcining Bones
Bone ash is the white material left when bones are calcined: mainly calcium phosphate, generally given as Ca5(OH)(PO4)3, about 56% calcium oxide and 42% phosphorus pentoxide by analysis. It melts only at about 1670 °C. Its porous, high-melting structure makes it the classic cupel for separating silver and gold from lead, and it forms about half of the body of bone china.
초급
Workshop process
안내
1
1
Clean the bones
Clean the bones
Remove any meat from the bones, then degrease them.
이 단계의 재료:
뼈1 as required필요한 도구:
칼2
2
Calcine
Calcine
Calcine the bones in a kiln. For bone china they are calcined to around 1000 °C (up to about 1100 °C), which removes all organic matter and leaves the bone sterilised and white; traditional bone ash was calcined lower, at around 800 °C. Most bones keep their cellular structure through calcination. Handle the hot bones with tongs and heat-resistant gloves, and let them cool before grinding.
필요한 도구:
가마(킬른)
부집게
내열 장갑3
3
Grind
Grind
Grind the calcined bone with water to a fine particle size, then partially dewater it.
이 단계의 재료:
물1 as required필요한 도구:
막자사발과 막자이 블루프린트로 만드는 것
관련 블루프린트
이 블루프린트들은 지식을 공유합니다 — 기술, 재료 또는 원리
CC0 퍼블릭 도메인
이 블루프린트는 CC0로 공개되었습니다. 어떤 목적으로든 자유롭게 복사, 수정, 배포 및 사용할 수 있습니다.
제품 구매를 통해 메이커를 지원하세요. 판매자가 설정한 메이커 커미션 을 받거나, 이 블루프린트의 새로운 반복을 만들어 연결로 포함시킬 수 있습니다.