Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)
Extruded polystyrene foam blown with a mix of methyl chloride and methylene chloride. Polystyrene soaks up both under pressure at 60 °C into a gel. The gel is heated to 90 °C and let out through the bottom valve, where it swells into foam. The gel flowed rapidly and gave small cells that did not shrink or collapse. McIntire found that a hotter gel gives finer cells, because the heat boils off all the chlorides. Methyl chloride is a toxic, flammable gas.
Source: O. R. McIntire (Dow), US 2,450,436 (1948), Example 2. Picture: the patent's drawing.
고급
3 days
이 블루프린트로 만드는 것
관련 블루프린트
이 블루프린트들은 지식을 공유합니다 — 기술, 재료 또는 원리

위험
Extruded Polystyrene Foam Board: Polystyrene Swollen with Methyl Chloride and Let Out below 130 °C
Charlie 작성
산업용
11
0
0
0
0
0

위험
Dichloromethane: Chloroform Reduced with Zinc, Alcohol and Hydrochloric Acid (Greene, in Thorpe 1912)
Charlie 작성
산업용
13
0
0
0
0
0

위험
Methyl Chloride: Hydrogen Chloride into Boiling Methanol over Zinc Chloride, Groves 1874
Charlie 작성
유기
13
0
0
0
0
0
CC0 퍼블릭 도메인
이 블루프린트는 CC0로 공개되었습니다. 어떤 목적으로든 자유롭게 복사, 수정, 배포 및 사용할 수 있습니다.
제품 구매를 통해 메이커를 지원하세요. 판매자가 설정한 메이커 커미션 을 받거나, 이 블루프린트의 새로운 반복을 만들어 연결로 포함시킬 수 있습니다.