Technical Molybdic Oxide: Molybdenite Roasted in Nichols-Herreshoff Furnaces (US Bureau of Mines 1957)

Molybdenite concentrate is roasted in air in a multiple-hearth furnace: it dries on the top hearth at 300 °F and roasts on the lower hearths at up to 1,250 °F, coming out about 4 hours later as molybdic oxide. Result: technical molybdic oxide with 0.06 to 0.30 % sulphur, packed in cans or bags for the steel industry. Source: US Bureau of Mines Information Circular 7784, Molybdenum - A Materials Survey (1957), p. 37, practice of Molybdenum Corporation of America at Washington, Pa. Not given: feed rate, air, fuel, yield. The sulphur leaves as sulphur dioxide, a poisonous gas. Picture drawn by Youblob.
고급
4 hours

위험 콘텐츠

이 블루프린트에는 위험한 절차가 포함되어 있습니다. 단계별 지침을 보려면 로그인하고 계정 설정에서 위험한 콘텐츠를 활성화하세요.

로그인

이 블루프린트로 만드는 것

CC0 퍼블릭 도메인

이 블루프린트는 CC0로 공개되었습니다. 어떤 목적으로든 자유롭게 복사, 수정, 배포 및 사용할 수 있습니다.

제품 구매를 통해 메이커를 지원하세요. 판매자가 설정한 메이커 커미션 을 받거나, 이 블루프린트의 새로운 반복을 만들어 연결로 포함시킬 수 있습니다.

토론

(0)

로그인 하여 토론에 참여하세요

댓글 로딩 중...