Water-Cooled Copper Mould: Two Halves with Cast-In Pipes, in a Trunnion Yoke (Peirce, US 2,048,024, 1936)
A mould for metals that conduct heat well: two thick copper blocks, each cast round a grid of copper pipes that carry cooling water. They are bolted face to face, so the cavity can be machined accurately, and carried in a steel yoke on hollow trunnions that feed the water. A latched gate closes the bottom. The casting can be dumped out of the top by turning the yoke, or out of the bottom by opening the gate.
Result: a water-cooled copper mould that freezes the metal fast and can be taken apart, machined and cleaned.
Source: W. H. Peirce (American Smelting and Refining), US 2,048,024 (1936). Unknown: sizes and the copper grade. Picture: the patent drawing.
උසස්
Unknown
උපදෙස්
1
1
Cast the two halves round their pipes
Cast the two halves round their pipes
For each half, assemble copper pipes into a grid: a horizontal inlet pipe at the bottom, an outlet pipe at the top, and several vertical pipes joining them. Any steam formed in casting then rises to the outlet. Cast a block of copper of about the mould's shape over the grid. Ours: copper ingot melted in a crucible furnace. Not given: sizes, the copper grade.
මෙම පියවර සඳහා ද්රව්ය:
තඹ නළය1 cooling-pipe grids
තඹ වාත්තු කැටය1 mould blocksඅවශ්ය මෙවලම්:
මූෂා උදුන
නොදන්නා මිනුම්2
2
Machine the cavity
Machine the cavity
Machine the inner faces of the two halves to form the casting space, accurately. The recesses can be cut to different depths, for example five-eighths of the casting's width in one half and three-eighths in the other. Bolt the halves together face to face.
මෙම පියවර සඳහා ද්රව්ය:
නොදන්නා ලෝහය1 boltsඅවශ්ය මෙවලම්:
මිලින යන්ත්රය
ස්ථාවර සිදුරු යන්ත්රය
ඉස්කුරුප්පු කැපීමේ කට්ටලය3
3
Make the yoke and the bottom gate
Make the yoke and the bottom gate
Cast a U-shaped steel yoke in one piece: two hollow ends with trunnions in line, joined by struts that carry the mould, bolted on. Make a bottom gate machined to fit tight under the mould, with its own cooling passage. Mount it on a gate arm keyed to a shaft across the yoke, its wedge end pinned in a V slot so the gate rocks to align. Add a lever on the shaft and a latch on an eccentric with a handle, to lock the gate up tight. Ours: steel ingot for the yoke casting.
මෙම පියවර සඳහා ද්රව්ය:
වානේ කැටය1 yoke casting
නොදන්නා ලෝහය1 gate, arm, shaft, lever, latchඅවශ්ය මෙවලම්:
මූෂා උදුන
මිලින යන්ත්රය4
4
Pipe the cooling water
Pipe the cooling water
Bring water in through a pipe in the centre of one trunnion into the hollow yoke end, and from there by fitted pipes to the inlets of both halves and by a flexible metal hose to the gate. Lead the outlets to the other hollow end, and out through a pipe in the centre of the other trunnion, so the water keeps flowing while the yoke turns. Not given: the hose, the flow.
මෙම පියවර සඳහා ද්රව්ය:
තඹ නළය1 inlet and outlet pipes
නොදන්නා ද්රව්යය1 metallic hosesඅවශ්ය මෙවලම්:
ජලය5
5
Cast and dump a cake
Cast and dump a cake
Latch the gate shut, coat the cavity with a mould dressing such as graphite, circulate the water and fill the mould with molten metal. When the cake has cooled, turn the yoke on its trunnions so it slides out of the top, or trip the latch so the gate swings back and it drops out of the bottom. Unbolt the halves now and then to clean them or machine their faces true again.
අවශ්ය මෙවලම්:
ග්රැෆයිට් කුඩු
ජලයද්රව්ය
5- 1 inlet and outlet pipesස්ථානගත
- 1 mould blocksස්ථානගත
- 1 gate, arm, shaft, lever, latchස්ථානගත
- 1 yoke castingස්ථානගත
- 1 metallic hosesස්ථානගත
සම්බන්ධිත සැලසුම්වල ද්රව්ය

අනතුරුදායක
10% ආරෝපණය
Electrolytic Copper and Refinery Slimes: Blister Anodes Dissolved in Bluestone and Acid (Barnett, in Peters 1905)
Charlie විසින්
ලෝහ වැඩ
6
0
0
0
1
0

10% ආරෝපණය
Copper and Brass Tube Drawn from Strip
Forge විසින්
ලෝහ වැඩ
45
0
0
0
3
0

10% ආරෝපණය
Crucible Furnace: the Brass Founder's Sunk Coke Air Furnace (Larkin, 1907)
Forge විසින්
උදුන
7
0
0
0
1
0

10% ආරෝපණය
Universal Milling Machine
Martin විසින්
ශිල්පය
53
0
0
0
1
0

10% ආරෝපණය
Graphite Powder Ground from Plumbago
Mary විසින්
අකාබනික
13
0
0
0
2
0
මෙම සැලසුම සාදන්නේ
CC0 පොදු වසම
මෙම බ්ලූප්රින්ට් CC0 යටතේ නිකුත් කර ඇත. ඔබට අවසර නොමැතිව පිටපත් කිරීම, වෙනස් කිරීම, බෙදා හැරීම සහ භාවිතා කිරීම කළ හැක.
බ්ලූප්රින්ට් හරහා නිෂ්පාදන මිලදී ගැනීමෙන් නිර්මාතෘට සහාය වන්න නිර්මාතෘ කොමිසම විකුණුම්කරුවන් විසින් නියම කළ, හෝ මෙම බ්ලූප්රින්ට්හි නව අනුවාදයක් සාදා ආදායම බෙදා ගැනීමට ඔබේ බ්ලූප්රින්ට්හි සම්බන්ධතාවයක් ලෙස ඇතුළත් කරන්න.